Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.   

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type   

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

40 40 H40

40*40*40(mm)

Panel size available:

1247*4047,1007*4047,1007*3007 

Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:40

Open Aera:67%

Approx Weight:19.2kgs/m²

Liner load

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4007.3197.14
Uniform load

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.81007.14
6007.7458.55
40 40 H40

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

40 40 H40
40 40 H40
40 40 H40

Application Scenarios

FRP molded grating 40*40H40 is suitable for platforms, walkways, trench covers and equipment operating surfaces that require corrosion resistance, slip resistance and load-bearing capacity. It is commonly used in chemical, water treatment, power and marine engineering environments. For suitability under specific working conditions, we recommend confirming with us based on the medium, load and installation method.

Selection Guidance

During selection, factors such as the resin system, grating thickness, mesh size and support span can be considered comprehensively. For example, in corrosive medium environments, priority can be given to the corrosion-resistant resin type, while in areas with higher load-bearing requirements, attention can be paid to the grating height and support conditions. You are welcome to contact us, and our technical staff will provide selection advice and detailed specifications based on your actual working conditions.

Product Advantages

The molded process forms the grating as a whole, with uniform distribution of fibers and resin. It features light weight and high strength, corrosion resistance, slip resistance, and easy cutting and installation, which facilitates on-site processing and later maintenance. Compared with traditional metal materials, it helps extend the service life in humid and corrosive environments.

Inquiry Guidance

If you need to know the detailed specifications, colors, surface forms and commercial terms of FRP molded grating 40*40H40, you are welcome to contact us for detailed specifications and quotations. Please provide information such as the usage environment, load-bearing requirements and quantity, and we will recommend a suitable solution accordingly.

Operating Environment

  • This molded FRP grating is built for service in corrosive chemical environments, where its unsaturated polyester resin and glass fiber reinforcement resist degradation from acids, alkalis and salts.
  • It is suited to both indoor and outdoor installations, including industrial plants, walkways and platforms exposed to weather and repeated washdown.
  • With flame-retardant resin options, the grating supports use in areas where fire safety is a consideration, such as chemical processing and other industrial settings.
  • It performs in humid and wet conditions where traditional metal grating would corrode; for specific temperature, chemical exposure or load requirements, contact us for the full parameter list.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送