Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type
38 152 H38 Stair tread

38*152*38(mm)

Panel size available:

580*3660,610*3660 Bidirectional force       

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:38

Open Aera:65%

Approx Weight:17kgs/m²

38 152 H38 Stair tread

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns


Software - Sample 2 for three columns


Software - Sample 3 for three columns



应用场景

本产品适用于楼梯踏步、平台、走道等需要防滑、耐腐蚀和承重的场合,常见于化工、电力、水处理、海洋工程等行业。玻璃钢模塑格栅的轻质高强特性使其也适合对重量敏感或需频繁拆卸的作业环境。

选型指导

选型时需考虑承载要求、使用环境的腐蚀性、防滑需求及安装方式等因素。不同树脂类型在耐腐蚀和阻燃性能上各有侧重,可根据具体工况选择。欢迎联系我们获取详细规格与选型建议。

产品优势

玻璃钢模塑格栅具有重量轻、强度高、耐腐蚀、防滑、绝缘及免维护等优点,其表面凹槽设计能有效防滑,且可定制颜色以匹配现场环境。与传统金属格栅相比,在腐蚀性环境中使用寿命更长,综合成本更低。

询盘引导

如需了解更多产品信息、获取样品或定制方案,欢迎联系我们,我们将根据您的需求提供详细规格与报价。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数