玻璃钢模塑格栅25*100H25标准负载型
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 |
Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*25(mm)
Panel size available:
1220*3660 Length stress\Width stress
Bearing bar thickness (Top/Bottom):6.5/5.0
Bearing bar center:25
Open Aera:67%
Approx Weight:13.83kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅25*100H25标准负载型适用于一般工业平台、走道、沟盖板及设备操作面等需要防滑、耐腐蚀且承载要求适中的场合。在化工、水处理、电镀等存在一定腐蚀介质的环境中,该规格可作为常见选型之一,具体适配性欢迎联系我们结合实际工况确认。
选型指导
选型时可结合树脂体系、格栅厚度与网格尺寸匹配使用环境的腐蚀等级与荷载需求:25mm厚、100mm网格的规格侧重标准负载与常规防滑。若涉及特殊介质、高温或更高承载要求,建议提供工况参数,我们可协助推荐更合适的树脂类型与结构方案,欢迎联系我们获取详细规格与报价。
产品优势
该模塑格栅由不饱和聚酯树脂与无碱玻璃纤维在定制模具中整体成型,具备轻质高强、耐腐蚀、防滑及绝缘等玻璃钢材料的共性特点。模塑工艺使纵横纤维连续分布,抗冲击与整体性较好,同时便于切割安装,有助于降低后续维护工作量。
询盘引导
如需了解玻璃钢模塑格栅25*100H25标准负载型的规格参数、树脂选型或供货信息,欢迎联系我们获取详细规格与报价,我们将根据您的实际应用场景提供针对性的产品建议与技术支持。