    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Hook plate

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Hook plate

A*B*T


A*B*T



9*70*3.2(Hypotenuse)0.48

1" x 1" x 1/8" (Hypotenuse)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Fillet30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Fillet30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right angle30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Fillet30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right angle30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

钩子板作为乙烯基结构型材的配套件,常用于玻璃钢格栅、平台、走道及护栏等需要连接固定的部位。其造型便于与型材面贴合,适合在腐蚀性环境或户外工况下配合 FRP 结构使用。具体适用工况欢迎联系我们确认。

选型指导

选型时请结合所连接型材的截面尺寸、安装角度及受力方向,对照上方规格表中的 A*B*T 尺寸与重量参数进行匹配。若不确定对应型号,欢迎提供图纸或使用环境,我们可协助推荐合适规格。

产品优势

该钩子板采用玻璃纤维增强材料与树脂体系拉挤成型,具备 FRP 型材常见的轻质、耐腐蚀和绝缘特性,表面经包覆增强层处理,适合长期暴露于潮湿或化学介质环境。与金属连接件相比,有助于减少锈蚀带来的维护需求。