拉挤格栅 T-3320
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 33%
Approx Weight (With three-core shoots): 20.27kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 600 | --- | 0.25 | 0.51 | 1.02 | 1.78 | 3.3 | 16876 |
| 900 | 0.51 | 0.76 | 1.27 | 2.29 | 4.57 | 9.4 | 7492 |
| 1200 | 1.02 | 1.52 | 2.29 | 4.83 | 9.91 | 19.6 | 4215 |
| 1500 | 1.78 | 2.79 | 4.57 | 9.14 | 18.3 | 36.6 | 2696 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 600 | 0.25 | 0.51 | 0.76 | 1.52 | 2.03 | 4.06 | 55368 |
| 900 | 0.76 | 1.52 | 3.05 | 5.59 | 7.73 | 15 | 36895 |
| 1200 | 2.29 | 4.57 | 9.4 | --- | --- | --- | 27659 |
| 1500 | 5 | 9.91 | --- | --- | --- | --- | 22137 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 T-3320 适用于对承载与耐腐蚀有要求的工业平台、走道、沟盖板及设备操作面等场合。若您的工况涉及特定介质、温度或荷载条件,欢迎联系我们沟通具体使用环境。
选型指导
选型时需综合考虑树脂类型(如邻苯、间苯、乙烯基或酚醛等)、承载条规格、格栅厚度与网格尺寸,以及安装支撑跨距等因素。请将您的使用环境与承载需求告知我们,我们将协助您确认合适的配置方案。
产品优势
拉挤格栅以拉挤型材作承载条,具有较高的纵向强度与刚度,重量轻、耐腐蚀、便于切割安装,并可减少维护需求。相较于传统金属格栅,其在潮湿、酸碱等腐蚀性环境中更具适应性。
询盘引导
如需了解拉挤格栅 T-3320 的详细规格、树脂体系选择与报价信息,欢迎联系我们,我们将根据您的项目需求提供相应支持。