结构型材-T型钢(邻苯)

结构型材-T型钢(邻苯)

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

T-shaped steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

T-shaped steel

A*B*T


A*B*T



54*6*31*6

0.89

9/4" x 1/4" x 19/16" x 1/4"

1.96

54*5*45*6

1.03

9/4" x 3/16" x 7/4" x 1/4"

2.27

54*6*45*6

1.1

9/4" x 1/4" x 7/4" x 1/4"

2.43

60*6*46*6

1.3

19/8" x 1/4" x 19/16" x 1/4"

2.87

78*6.4*44.5*6

1.38

3" x 1/4" x 7/4" x 1/4"

3.04

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar 

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

T型钢(邻苯)作为结构型材,常用于需要高强度和较大跨度的支撑、框架与加强结构,如平台护栏、走道骨架、设备支架及腐蚀环境下的承重构件。其耐腐蚀、轻质高强的特点,使其适用于化工、水处理、海洋工程等对耐候性要求较高的场合。具体适用工况欢迎联系我们获取详细建议。

选型指导

选型时可依据结构跨度、荷载条件、连接方式及安装环境,结合T型钢的截面尺寸与单位重量进行匹配。邻苯树脂体系在耐腐蚀与力学性能之间具有均衡表现,适合多数通用结构需求。如不确定选用哪种规格,欢迎联系我们获取详细规格与报价,由技术人员协助确认。

产品优势

该T型钢以玻璃纤维为增强材料、树脂为粘结剂,经拉挤成型工艺制成,具有轻质高强、耐腐蚀、绝缘无磁等特性,便于切割与现场安装。相比传统金属型材,它在潮湿或腐蚀性环境中更易维护。如需了解具体性能数据,欢迎联系我们获取详细规格与报价。

询盘引导

如需获取T型钢(邻苯)的详细规格、尺寸公差、供货形式及商务条款,欢迎联系我们。请提供所需规格、数量与使用环境,我们将尽快回复并提供报价与技术支持。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数