FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
| 1000*50.8*4 | 9.1 | 39" x 2" x 3/16" | 20.1 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Large corrugated sheets are commonly used for roof and wall cladding of industrial plants, warehouses, chemical plants, sewage tanks and similar buildings. They can also be used for outdoor sun shading, canopies and equipment protective covers with high corrosion resistance requirements. The vinyl resin provides good chemical corrosion resistance and weather resistance, making it suitable for corrosive gas or humid environments. To learn about suitability for specific working conditions, please contact us for detailed specifications and recommendations.
Selection Guide
During selection, load, span, support spacing and the corrosion level of the service environment should be considered comprehensively to determine the appropriate sheet thickness, corrugation and length. Large corrugated sheets usually adapt to different spans by adjusting overlap and fixing methods. Structural calculation by a professional engineer is recommended. We can provide customized solutions based on your project requirements. Please contact us for detailed specifications and quotations.
Product Advantages
This product uses glass fiber reinforced vinyl resin and is pultruded, featuring light weight, high strength, corrosion resistance, aging resistance and adjustable light transmission (requiring corresponding additives), and is easy to cut and install with low maintenance cost. Compared with metal sheets, it has a longer service life in corrosive environments and good insulation performance. To compare with other materials or learn specific performance data, please contact us for detailed specifications and quotations.
Inquiry Guide
To obtain detailed technical parameters, samples or quotations for large corrugated sheets, please provide your specific application scenario, dimension requirements and quantity. Our technical team will provide selection support. Please contact us for detailed specifications and quotations.
Operating Environment
- This molded vinyl ester FRP corrugated structural profile is designed for both indoor and outdoor installations, including industrial plants, chemical processing areas, and architectural applications where the material's vinyl ester resin matrix provides resistance to moisture and humidity.
- The vinyl ester resin used in this FRP structural shape offers enhanced tolerance to a range of corrosive media, including many acids, alkalis, and salt solutions, making it suitable for environments where steel or other metals would degrade rapidly.
- Typical service conditions include exposure to temperature fluctuations; the material's physical properties are stable across common ambient and industrial operating temperature ranges, though specific limits depend on the exact chemical environment and load requirements.