    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

I-beam

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

I-beam

A*B*T1*T2


A*B*T1*T2


IB32

15*32*6.4*4

0.51

9/16" x 5/4" x 1/4" x 3/16"

1.12

IB38A

30*38*3*3

0.53

19/16" x 3/2" x 1/8" x 1/8"

1.17

IB45A

45*9*180*12

5.4

7/4" x 3/8" x 7" x 1/2"

11.9

IB50A

50*102*6.4*6.4

2.4

2" x 4" x 1/4" x 1/4"

5.29

IB50B

50*102*8*8

3

2" x 4" x 5/16" x 5/16"

6.61

IB76A

76*152*6.4*6.4

3.59

3" x 6" x 1/4" x 1/4"

7.91

IB76B

76*152*9.5*9.5

5.32

3" x 6" x 3/8" x 3/8"

11.73

IB102A

102*203*9.5*9.5

7.2

4" x 8" x 3/8" x 3/8"

15.87

IB102B

102*203*12.7*12.7

9.5

4" x 8" x 1/2" x 1/2"

20.94

IB120

120*240*12*12

10.5

19/4" x 19/2" x 1/2" x 1/2"

23.15

IB127A

127*254*9.5*9.5

9

5" x 10" x 3/8" x 3/8"

19.84

IB127B

127*254*12.7*12.7

11.9

5" x 10" x 1/2" x 1/2"

26.24

IB127C

127*152*9.5*9.5

7.1

5" x 6" x 3/8" x 3/8"

15.65

IN127D

127*152*12.7*12.7

9.2

5" x 6" x 1/2" x 1/2"

20.28

IB152A

152*305*9.5*9.5

10.7

6" x 12" x 3/8" x 3/8"

23.68

IB152B

152*305*12.7*12.7

14.3

6" x 12" x 1/2" x 1/2"

31.53

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Vinylester I-beams are suitable for high-humidity, highly corrosive and high-strength environments, such as chemical platforms, wastewater treatment facilities, marine engineering and power facilities. Their lightweight, high-strength characteristics facilitate transportation and installation, making them suitable for large-span structures. Contact us to learn about specific application cases.

Selection Guide

Selection requires comprehensive consideration of load, span, corrosive environment and installation conditions. It is recommended to determine the beam cross-section dimensions based on design loads and support spacing, and to select the appropriate model with reference to the product specification table. For technical support, contact us for selection advice.

Product Advantages

Vinylester I-beams offer excellent corrosion resistance, high strength and lightweight characteristics, along with good insulation and aging resistance. Compared with steel, they have a longer service life and lower maintenance costs. Contact us for detailed performance data.

Inquiry Guidance

For more product specifications, prices or customization requirements, contact us for detailed specifications and quotations. Our technical team will provide you with professional support.

Operating Environment

  • These vinyl resin FRP I-beams are drawn as pultruded structural shapes, so the finished profile is suited to outdoor service as well as indoor installation, including structures that see direct weather exposure.
  • The glass fiber reinforcement and vinyl resin matrix make the I-beam a candidate for chemically aggressive surroundings such as plant areas with acid or alkali vapours, splash zones and humid process rooms, where the profile is chosen for its corrosion resistance rather than for steel.
  • Because the section is pultruded in a heated metal mold and cured before pulling, the beam keeps its shape in humid or wet conditions and in wide temperature swings between cold and hot plant environments.
  • Typical placements for this I-beam line are load-bearing frames, spans and supports in wastewater, chemical, cooling tower and other processing facilities where moisture and corrosive media are present.