FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in)
| Weight(lbs/in) |
I-beam | A*B*T1*T2 | A*B*T1*T2 | ||
| IB32 | 15*32*6.4*4 | 0.51 | 0.59*1.26*0.25*0.16 | 1.12 |
| IB38A | 30*38*3*3 | 0.53 | 1.18*1.5*0.12*0.12 | 1.17 |
| IB45A | 45*9*180*12 | 5.4 | 1.77*0.35*7.09*0.47 | 11.9 |
| IB50A | 50*102*6.4*6.4 | 2.4 | 1.97*4.02*0.25*0.25 | 5.29 |
| IB50B | 50*102*8*8 | 3 | 1.97*4.02*0.31*0.31 | 6.61 |
| IB76A | 76*152*6.4*6.4 | 3.59 | 2.99*5.98*0.25*0.25 | 7.91 |
| IB76B | 76*152*9.5*9.5 | 5.32 | 2.99*5.98*0.37*0.37 | 11.73 |
| IB102A | 102*203*9.5*9.5 | 7.2 | 4.02*7.99*0.37*0.37 | 15.87 |
| IB102B | 102*203*12.7*12.7 | 9.5 | 4.02*7.99*0.5*0.5 | 20.94 |
| IB120 | 120*240*12*12 | 10.5 | 4.02*9.45*0.47*0.47 | 23.15 |
| IB127A | 127*254*9.5*9.5 | 9 | 5*10*0.37*0.37 | 19.84 |
| IB127B | 127*254*12.7*12.7 | 11.9 | 5*10*0.5*0.5 | 26.24 |
| IB127C | 127*152*9.5*9.5 | 7.1 | 5*5.98*0.37*0.37 | 15.65 |
| IN127D | 127*152*12.7*12.7 | 9.2 | 5*5.98*0.5*0.5 | 20.28 |
| IB152A | 152*305*9.5*9.5 | 10.7 | 5.98*12.01*0.37*0.37 | 23.68 |
| IB152B | 152*305*12.7*12.7 | 14.3 | 5.98*12.01*0.5*0.5 | 31.53 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-工字梁适用于对强度与跨距有要求的承重与支撑部位,例如平台走道、栈桥、设备支架、护栏骨架及腐蚀性环境中的结构框架。不同树脂体系与纤维铺层可适配多种工况,欢迎联系我们获取详细规格与报价。
选型指导
选型时需综合考虑载荷形式、跨距、支撑条件、使用环境及连接方式,据此确定截面尺寸与长度方向的要求。由于各工况差异较大,建议提供使用条件由我方协助确认合适型号,欢迎联系我们获取详细规格与报价。
产品优势
FRP工字梁以玻璃纤维增强材料与树脂复合而成,具有轻质高强、耐腐蚀、绝缘无磁、易于切割与现场加工等特点,便于在金属型材易锈蚀的场合替代使用。具体性能表现随配方与规格而变,欢迎联系我们获取详细规格与报价。
询盘引导
如需确认截面规格、长度、颜色、树脂类型或配套连接方案,请提供图纸或使用条件,我方将据此给出建议。欢迎联系我们获取详细规格与报价,也可就样品与批量供货事宜进一步沟通。