FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Hook plate | A*B*T | A*B*T | ||
| 9*70*3.2(Hypotenuse) | 0.48 | 1" x 1" x 1/8" (Hypotenuse) | 1.06 | |
| 25*60*3 | 0.5 | 1" x 19/8" x 1/8" | 1.1 | |
| 25*50*3(75°) | 0.45 | 1" x 2" x 1/8" (75°) | 0.99 | |
| 30*70*4(90°) | 0.75 | 19/16" x 11/4" x 3/16" (90°) | 1.65 | |
| 30*70*3.2(90°) | 0.7 | 19/16" x 11/4" x 1/8" (90°) | 1.54 | |
| 30*90*3(87°) | 0.72 | 19/16" x 7/2" x 1/8" (87°) | 1.59 | |
| 38*230*3.2(87°) | 1.65 | 3/2" x 9" x 1/8" (87°) | 3.64 | |
| 40*254*6.4(87°) | 3.55 | 25/16" x 10" x 1/4" (87°) | 7.83 | |
| 50*140*3.2(87°) | 1.19 | 2" x 11/2" x 1/8" (87°) | 2.62 | |
| 55*152*3.6(87°) | 1.55 | 9/4" x 6" x 1/8" (87°) | 3.42 | |
| 55*230*3.6(87°) | 2.14 | 9/4" x 9" x 1/8" (87°) | 4.72 | |
| 55*205*3.2(87°) | 1.62 | 9/4" x 8" x 1/8" (87°) | 3.57 | |
| 55*55*3.2(87°) | 0.8 | 9/4" x 9/4" x 1/8" (87°) | 1.76 | |
| 55*70*3.2(87°) | 0.9 | 9/4" x 11/4" x 1/8" (87°) | 1.98 | |
| 30*76*3 | 0.6 | 19/16" x 3" x 1/8" | 1.32 | |
| 30*76*4 | 0.8 | 19/16" x 3" x 3/16" | 1.76 | |
| 25*50*3.2(90°) | 0.45 | 1" x 2" x 1/8" (90°) | 0.99 | |
| 25*50*4(90°) | 0.51 | 1" x 2" x 3/16" (90°) | 1.12 | |
| 25*100*3.2(87°) | 0.75 | 1" x 4" x 1/8" (87°) | 1.65 | |
| Fillet | 30*75*3.5 | 0.69 | 19/16" x 3" x 1/8" | 1.52 |
| Fillet | 30*100*3.2 | 0.8 | 19/16" x 4" x 1/8" | 1.76 |
| Right angle | 30*100*3.2 | 0.85 | 19/16" x 4" x 1/8" | 1.87 |
| 30*152*3.2 | 1.2 | 19/16" x 6" x 1/8" | 2.65 | |
| Fillet | 30*230*3.2 | 1.6 | 19/16" x 9" x 1/8" | 3.53 |
| Right angle | 30*230*3.2 | 1.7 | 19/16" x 9" x 1/8" | 3.75 |
| 55*300*4(90°) | 2.8 | 9/4" x 12" x 3/16" (90°) | 6.17 | |
| 55*345*4(87°) | 3.25 | 9/4" x 27/2" x 3/16" (87°) | 7.17 | |
| 30*381*3.2(87°) | 2.7 | 19/16" x 15" x 1/8" (87°) | 5.95 | |
| 55*400*3.2 | 2.8 | 9/4" x 63/4" x 1/8" | 6.17 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
FRP钩子板常用于化工、污水处理、海洋工程等腐蚀性环境中的结构支撑与连接,也适用于需要绝缘、无磁性的场合。其安装方式灵活,可根据实际工况进行切割、钻孔等加工。
选型指导
选型时需考虑荷载要求、跨度、腐蚀环境及连接方式等因素。建议根据具体项目需求确定尺寸与规格,欢迎联系我们获取详细规格与选型建议。
产品优势
FRP钩子板具有轻质高强、耐腐蚀、绝缘无磁、安装便捷等特点,相比传统金属材料可显著降低维护成本。