结构型材-H梁
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in)
| Weight(lbs/in) |
H beam | A*B*T1*T2 | A*B*T1*T2 | ||
| HB76 | 76*76*6.4*6.4 | 2.67 | 2.99*2.99*0.25*0.25 | 5.73 |
| HB102A | 102*102*6.4*6.4 | 3.59 | 4.02*4.02*0.25*0.25 | 7.91 |
| HB102B | 102*102*8*8 | 4.5 | 4.02*4.02*0.31*0.31 | 9.92 |
| HB152A | 152*152*6.4*6.4 | 5.43 | 5.98*5.98*0.25*0.25 | 11.97 |
| HB152B | 152*152*9.5*9.5 | 8.1 | 5.98*5.98*0.37*0.37 | 17.86 |
| HB203A | 203*203*9.5*9.5 | 10.8 | 7.99*7.99*0.37*0.37 | 23.81 |
| HB203B | 203*203*12.7*12.7 | 14.4 | 7.99*7.99*0.5*0.5 | 31.66 |
| HB203C | 203*203*6.4*6.4 | 7.5 | 7.99*7.99*0.25*0.25 | 16.53 |
| HB254A | 254*254*9.5*9.5 | 13.6 | 10*10*0.37*0.37 | 29.98 |
| HB254B | 254*254*12.7*12.7 | 18 | 10*10*0.5*0.5 | 39.77 |
| HB305 | 305*305*12.7*12.7 | 21.5 | 12.01*12.01*0.5*0.5 | 47.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² |
316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
FRP H梁常用于对强度、耐腐蚀与绝缘有要求的承载结构,如平台框架、走道支撑、桥架与化工、水处理、海洋等腐蚀性环境中的梁柱构件。其轻质高强的特点适合大跨度与需要减少维护的场合,欢迎联系我们获取详细规格与报价。
选型指导
选型时可结合跨度、荷载条件、安装方式及使用环境,对照A×B×T1×T2的截面尺寸与单位重量综合评估。若不确定合适规格,欢迎联系我们,由技术团队协助确认详细规格与报价。
产品优势
FRP H梁以玻璃纤维增强材料与树脂拉挤成型,具有轻质高强、耐腐蚀、绝缘及易于切割安装等特性,可减少后期维护。相比传统金属型材,更适合潮湿、酸碱等苛刻环境,欢迎联系我们获取详细规格与报价。
询盘引导
如需了解FRP H梁的截面规格、长度、颜色及配套连接方案,欢迎联系我们,我们将根据您的项目需求提供详细规格与报价。请告知使用环境与数量,以便我们更快响应。
简体中文