FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Flat | Thickness*Width | Thickness*Width | ||
FP32A | 3.2*1000 | 6.18 | 1/8" x 39" | 13.6 |
FP32B | 3.2*1220 | 7.42 | 1/8" x 48" | 16.4 |
FP40A | 4*800 | 6.2 | 3/16" x 32" | 13.7 |
FP40B | 4*1200 | 9.19 | 3/16" x 48" | 20.3 |
FP48 | 4.8*1000 | 9.3 | 3/16" x 39" | 20.5 |
FP50A | 5*440 | 4.25 | 3/16" x 17" | 9.37 |
FP50B | 5*1220 | 11.8 | 3/16" x 48" | 26 |
FP64 | 6.4*1220 | 14.84 | 1/4" x 48" | 32.7 |
FP95 | 9.5*1220 | 22.02 | 3/8" x 48" | 48.6 |
FP127 | 12.7*1220 | 29.44 | 1/2" x 48" | 64.9 |
FP160 | 16*1220 | 37.2 | 5/8" x 48" | 82 |
FP190 | 19*1220 | 44.1 | 3/4" x 48" | 97.2 |
FP254 | 25.4*1220 | 59 | 1" x 48" | 130 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profile - Flat Panel (Orthophthalic) is commonly used in high-strength, large-span structural applications, such as platform walkways, trench covers, railings and support frames, and other industrial environments requiring corrosion resistance and load-bearing capacity. If your working conditions involve acids, alkalis, moisture or outdoor exposure, please contact us with details of your service environment, and we can help assess suitability.
Selection Guide
When selecting, it is recommended to first clarify the thickness and width of the flat panel, the span and support method, as well as the load type (concentrated or uniformly distributed) and corrosive media, and then determine the specifications according to the installation direction and fixing method. Different sizes offer different load-bearing performance. For specific thickness, width and load-bearing data, please contact us for detailed specifications and a quotation.
Product Advantages
This flat panel is made of glass fiber reinforced material compounded with resin and formed by molding/pultrusion. It combines good physical properties with corrosion resistance. It is relatively lightweight and easy to cut and install. Its surface is smooth and its insulation performance is good, making it suitable to replace some traditional metal plates in corrosive or electromagnetically sensitive environments.
Inquiry Guidance
If you need to know the detailed specifications, customized dimensions, packaging and delivery methods of Structural Profile - Flat Panel (Orthophthalic), please contact us for detailed specifications and a quotation. Please provide thickness, width, length, quantity and service environment, and we will recommend a suitable solution accordingly.
Operating Environment
- This pultruded FRP flat profile is built from glass fiber reinforcement with resin as the binder, so it is suited to both indoor installations and outdoor exposure where moisture and weather are present.
- The resin system and glass fiber reinforcement make the flat profile a practical choice for corrosive industrial surroundings, including chemical plants, wastewater treatment areas and coastal sites where steel would need frequent replacement.
- Because it is produced by drawing the resin-impregnated glass fiber through a heated metal mold, the flat profile keeps its shape in service and is typically used where high strength and large span conditions are required.
- For project-specific temperature, humidity and chemical exposure limits, contact us for the full parameter list of this flat profile line; the sizes shown in the table can be reviewed together with your operating conditions.