拉挤格栅 I-60125
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 32mm
Open Area: 60%
Approx Weight (With three-core shoots): 13.5kg/m²
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅具有轻质高强、耐腐蚀、防滑等特点,广泛应用于化工、石油、电力、海洋工程、污水处理等行业的操作平台、走道、地沟盖板及围栏。不同使用环境可根据树脂类型选择,如耐酸场合可选乙烯基树脂型,防火要求高的场合可选酚醛树脂型。
选型指导
选型时需考虑承载需求、跨距、使用环境腐蚀性及防火要求。格栅的承载条形状(I型、T型)和连接杆间距会影响承载能力,树脂类型决定耐腐蚀和阻燃性能。建议您提供具体使用条件,我们的技术团队将为您推荐合适方案。欢迎联系我们获取详细规格与技术支持。
产品优势
与传统金属格栅相比,拉挤格栅重量轻、耐腐蚀、绝缘、免维护,且安装方便。其独特的组装工艺保证了格栅的整体性和承载能力,可根据需要切割成不同尺寸。适用于对耐腐蚀和防火有较高要求的场合。
询盘引导
如需了解更多产品信息或获取定制方案,欢迎联系我们。请提供您的具体需求(如尺寸、承载要求、使用环境等),我们将尽快为您提供详细规格与报价。