玻璃钢模塑格栅83*83H25
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

Feature One

Feature Two

Feature Three

83*83*25(mm)
Panel size available:
1007*4007,1007*3007 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:83
Open Aera:84%
Approx Weight:5.8kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅83*83H25适用于对防腐蚀、轻质高强和防滑有要求的平台、走道、地沟盖板及设备操作面,常见于化工、水处理、电力与海洋工程等环境。其25mm厚度与83*83mm网格在承载与通透性之间取得平衡,适合中轻载荷的通行与排水场景。具体工况适配性欢迎联系我们结合现场条件确认。
选型指导
选型时可从载荷需求、跨距、腐蚀介质、阻燃要求与安装方式几个维度出发:树脂体系影响耐腐蚀与阻燃表现,格栅厚度与网格尺寸影响承载与自重,表面处理影响防滑与外观。若您提供使用环境与承载条件,我们可协助推荐合适的树脂类型与结构方案。详细规格与选型建议欢迎联系我们获取。
产品优势
模塑格栅采用树脂与玻璃纤维一体成型,具有轻质高强、耐腐蚀、不导电、免维护等通用优势,且网格结构利于透水透气、减少积污。相比传统金属格栅,其在潮湿或腐蚀性环境中更耐久,安装与切割也较为便捷。具体性能表现以实际选型与检测报告为准,欢迎联系我们了解更多。
询盘引导
如需获取玻璃钢模塑格栅83*83H25的详细规格、树脂选项、价格与交付信息,欢迎联系我们。请提供使用场景、承载要求、尺寸数量及特殊需求,我们将尽快为您提供针对性方案与报价。