Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Recommended usage occasions | |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

79*79*23(mm)
Panel size available:
405*3569 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.5/5.0
Bearing bar center:79
Open Aera:80%
Approx Weight:5.7kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅79*79H23具备耐腐蚀、轻质高强、防滑等特性,适用于化工、电镀、污水处理、海洋工程等腐蚀性环境中的操作平台、走道和地沟盖板。其79*79mm网格与23mm厚度设计兼顾承载与透水透气需求,也常见于对洁净度和安全性有要求的工业场所。具体工况适配建议欢迎联系我们沟通。
选型指导
选型时需结合实际载荷、跨距、支撑方式及腐蚀介质类型,确认格栅的树脂体系、厚度与网格尺寸是否匹配。本产品采用不饱和聚酯树脂与无碱玻璃纤维模压成型,可根据使用环境选择不同树脂类型以平衡耐腐蚀与阻燃要求。若您提供工况参数,我们可协助推荐合适规格,欢迎联系我们获取详细规格与报价。
产品优势
模塑格栅整体成型,纤维与树脂分布均匀,具有优良的耐腐蚀性和双向承载能力,且重量轻、便于切割安装,维护成本低。表面可做防滑处理,降低湿滑环境下的作业风险。相比传统金属格栅,其在酸碱盐环境中使用寿命更长,且无需频繁防腐维护。