玻璃钢模塑格栅40*40H30
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasion |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasion |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




40*40*30(mm)
Panel size available:
1247*4047,1007*4047,1007*3007
Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:40
Open Aera:67%
Approx Weight:14.6kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
Span( mm) | 75 | 150 | 300 | 450 | 750 | 1500 | Load |
| 300 | <0.25 | <0.25 | 0.26 | 0.51 | 0.76 | 1.53 | 9924 |
| 450 | 0.26 | 0.51 | 1.02 | 1.53 | 2.54 | 3.92 | 4828 |
| 600 | 0.51 | 1.27 | 2.29 | 3.56 | 5.85 | 7.38 | 4113 |
| 750 | 1.27 | 2.54 | 4.83 | 7.37 | 12.5 | 16 | 3174 |
| 900 | 2.27 | 4.54 | 9.08 | 13.7 | 18.8 | 22.1 | 2638 |

Uniform load(units:mm)
Deflcvtion |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
Span( mm) | 350 | 500 | 750 | 1000 | 1500 | 2500 |
| 300 | 0.29 | 0.48 | 0.57 | 0.75 | 1.15 | 1.82 |
| 450 | 0.78 | 1.19 | 1.81 | 2.47 | 3.54 | 5 |
| 600 | 1.76 | 2.66 | 4.28 | 5.56 | 8.41 | 13.2 |
| 750 | 3.48 | 5.12 | 8.21 | 11 | 16.5 | --- |
| 900 | 5.89 | 8.81 | 14.2 | 19 | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
玻璃钢模塑格栅40*40H30广泛应用于石油化工、电力、污水处理、海洋工程等领域的操作平台、走道、楼梯踏板及地沟盖板。其耐腐蚀、防滑、轻质高强的特性适合潮湿、酸碱等腐蚀性环境。如需了解在特定工况下的适用性,欢迎联系我们获取详细规格与报价。
选型指导
选型时需综合考虑承载要求、跨距、腐蚀环境及安全需求。不同树脂类型(如邻苯型、间苯型、乙烯基酯型、双酚A型)和厚度影响格栅的耐腐蚀性、阻燃性及力学性能。建议根据实际使用条件选择合适型号,欢迎联系我们获取详细规格与报价。
产品优势
玻璃钢模塑格栅具有优异的耐腐蚀性、 lightweight、高强度、防滑、绝缘及长寿命等特点。其表面凹槽或砂面设计提供良好防滑性能,且易于切割安装,维护成本低。如需了解具体性能数据,欢迎联系我们获取详细规格与报价。
询盘引导
如果您对玻璃钢模塑格栅40*40H30感兴趣或有特定需求,欢迎联系我们获取详细规格与报价。我们可提供定制化解决方案,满足您的项目要求。

简体中文