Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property |
Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*60(mm)
Panel size available:
1220*4000,1220*3660,1220*2440,
915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):11.5/9.0
Bearing bar center:38.1mm( 1.5")
Open Aera:54%
Approx Weight:50.4kgs/m²

Liner load(units:mm)
Span in (mm) |
Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 11.2 | 19 | 7.14 |

Uniform load(units:mm)
Span in (mm) |
Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 2.8 | 100 | 7.14 |
| 600 | 11.8 | 45 | 8.55 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
本产品为38×38mm网格、60mm厚度的重负载型玻璃钢模塑格栅,适用于需要高承载与耐腐蚀的工业平台、走道、地沟盖板及化工、污水处理、海洋工程等腐蚀性环境。若您的工况涉及强酸碱、潮湿或户外长期暴露,欢迎联系我们说明使用条件以获取适配建议。
选型指导
选型时请重点关注承载需求、跨距、支撑方式及腐蚀介质类型,并结合树脂体系(如邻苯型、间苯型、乙烯基型、双酚A型等)与表面防滑要求进行匹配。由于不同工况对厚度、网格尺寸及树脂选择的要求差异较大,欢迎提供图纸或工况参数,由我们协助确认合适规格。
产品优势
玻璃钢模塑格栅采用不饱和聚酯树脂与玻璃纤维整体模压成型,兼具轻质高强、耐腐蚀、防滑及绝缘等特性,且便于切割安装与后期维护。38×38mm网格与60mm厚度设计在保持通风透光的同时提供较高的承载能力,适合重载场合使用。
询盘引导
如需了解本产品的详细规格、树脂选项、颜色、表面处理及包装方式,欢迎联系我们获取详细规格与报价。请提供您的应用环境、承载要求与尺寸需求,我们将尽快为您推荐合适方案并回复商务条款。

简体中文
English