玻璃钢模塑格栅38*38H30 重负载型

玻璃钢模塑格栅38*38H30 重负载型

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

 Genius FRP

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38*38H30 Heavy duty

38*38*30(mm)

Panel size available:

1220*3660,1220*2440,915*3050

Bidirectional force. 

Bearing bar thickness (Top/Bottom):10.5/9.0

Bearing bar center:38

Open Aera:56% 

Approx Weight:25kgs/㎡ 

Liner load

Liner load(units:mm) 

Deflcvtion



kg/m




Limit

Span
(mm)

150

300

450

600

750

1500

Load

3000.360.480.610.760.891.0617116
6000.661.251.852.463.078.488718
9001.803.685.567.429.3013.85817
12004.759.6814.619.621.2---3755
Uniform load

Uniform load(units:mm)

Deflcvtion



kg/m²




Span
(mm)

240

480

980

1450

2450

3650

4880

3000.090.190.380.490.781.05---
6000.430.811.552.313.845.74---
9001.703.456.9610.4717.523.3---
12005.9712.224.532.638.7------
Software image and text block

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

38*38H30 Heavy duty
38*38H30 Heavy duty
38*38H30 Heavy duty

应用场景

玻璃钢模塑格栅38*38H30重负载型适用于需要较高承载能力与耐腐蚀性能的工业平台、走道、沟盖板及设备操作面等场合。其网格结构与树脂体系可适应化工、水处理、电力等存在潮湿或腐蚀性介质的环境,具体适配性建议结合工况联系我们确认。

选型指导

选型时请关注承载需求、支撑跨距、腐蚀介质类型及安装方式,并结合树脂体系与格栅厚度进行匹配。本产品为38*38mm网格、30mm厚度的重负载型模塑格栅,如需在不同载荷条件下对比选型,欢迎联系我们获取详细规格与技术支持。

产品优势

模塑格栅采用树脂与玻璃纤维整体成型,具有轻质高强、耐腐蚀、防滑及绝缘等特性,且便于切割与安装。重负载型结构在保持开孔率的同时提升了承载表现,适合对强度与耐久性有要求的应用环境。

询盘引导

如需了解玻璃钢模塑格栅38*38H30重负载型的详细规格、树脂体系选项及商务条款,欢迎联系我们获取详细规格与报价,我们将根据您的项目需求提供对应方案。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送