玻璃钢模塑格栅25*152H38

玻璃钢模塑格栅25*152H38

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 152 H38

25*152*38(mm)

Panel size available:

1220*3660,1220*2440,915*3050 Length stress      

Bearing bar thickness (Top/Bottom):9.0/6.5

Bearing bar center:25

Open Aera:63%

Approx Weight:22.5kgs/m²

25 152 H38

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

Software - Sample 1 for three columns


Software - Sample 2 for three columns


Software - Sample 3 for three columns



应用场景

玻璃钢模塑格栅25*152H38适用于对防滑、耐腐蚀和承载有要求的走道、平台、沟盖及设备操作面,常见于化工、水处理、电力和海洋工程等环境。具体场景是否适配,欢迎联系我们的技术团队沟通确认。

选型指导

选型时需关注树脂体系(如邻苯、间苯、乙烯基或双酚A型)、格栅厚度与网孔尺寸是否匹配荷载与介质条件,并可结合是否需阻燃、防滑面或特殊颜色来确认。由于涉及具体工况参数,建议您提供使用环境信息,由我们协助完成规格选择。

产品优势

该模塑格栅以不饱和聚酯树脂为基体、玻璃纤维增强,具有轻质高强、耐化学腐蚀、绝缘无磁及便于切割安装的特点,表面可做防滑处理。相比传统金属格栅,其在潮湿或腐蚀性环境中更利于长期使用与维护,具体性能表现视树脂与配方而定。

询盘引导

如需了解玻璃钢模塑格栅25*152H38的详细规格、适配方案与商务条款,欢迎联系我们获取详细规格与报价。请告知您的应用环境、所需尺寸与数量,我们将尽快为您提供选型建议与产品资料。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数