结构型材-钩子板(间苯)
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Hook plate | A*B*T | A*B*T | ||
| 9*70*3.2(Hypotenuse) | 0.48 | 1" x 1" x 1/8" (Hypotenuse) | 1.06 | |
| 25*60*3 | 0.5 | 1" x 19/8" x 1/8" | 1.1 | |
| 25*50*3(75°) | 0.45 | 1" x 2" x 1/8" (75°) | 0.99 | |
| 30*70*4(90°) | 0.75 | 19/16" x 11/4" x 3/16" (90°) | 1.65 | |
| 30*70*3.2(90°) | 0.7 | 19/16" x 11/4" x 1/8" (90°) | 1.54 | |
| 30*90*3(87°) | 0.72 | 19/16" x 7/2" x 1/8" (87°) | 1.59 | |
| 38*230*3.2(87°) | 1.65 | 3/2" x 9" x 1/8" (87°) | 3.64 | |
| 40*254*6.4(87°) | 3.55 | 25/16" x 10" x 1/4" (87°) | 7.83 | |
| 50*140*3.2(87°) | 1.19 | 2" x 11/2" x 1/8" (87°) | 2.62 | |
| 55*152*3.6(87°) | 1.55 | 9/4" x 6" x 1/8" (87°) | 3.42 | |
| 55*230*3.6(87°) | 2.14 | 9/4" x 9" x 1/8" (87°) | 4.72 | |
| 55*205*3.2(87°) | 1.62 | 9/4" x 8" x 1/8" (87°) | 3.57 | |
| 55*55*3.2(87°) | 0.8 | 9/4" x 9/4" x 1/8" (87°) | 1.76 | |
| 55*70*3.2(87°) | 0.9 | 9/4" x 11/4" x 1/8" (87°) | 1.98 | |
| 30*76*3 | 0.6 | 19/16" x 3" x 1/8" | 1.32 | |
| 30*76*4 | 0.8 | 19/16" x 3" x 3/16" | 1.76 | |
| 25*50*3.2(90°) | 0.45 | 1" x 2" x 1/8" (90°) | 0.99 | |
| 25*50*4(90°) | 0.51 | 1" x 2" x 3/16" (90°) | 1.12 | |
| 25*100*3.2(87°) | 0.75 | 1" x 4" x 1/8" (87°) | 1.65 | |
| Fillet | 30*75*3.5 | 0.69 | 19/16" x 3" x 1/8" | 1.52 |
| Fillet | 30*100*3.2 | 0.8 | 19/16" x 4" x 1/8" | 1.76 |
| Right angle | 30*100*3.2 | 0.85 | 19/16" x 4" x 1/8" | 1.87 |
| 30*152*3.2 | 1.2 | 19/16" x 6" x 1/8" | 2.65 | |
| Fillet | 30*230*3.2 | 1.6 | 19/16" x 9" x 1/8" | 3.53 |
| Right angle | 30*230*3.2 | 1.7 | 19/16" x 9" x 1/8" | 3.75 |
| 55*300*4(90°) | 2.8 | 9/4" x 12" x 3/16" (90°) | 6.17 | |
| 55*345*4(87°) | 3.25 | 9/4" x 27/2" x 3/16" (87°) | 7.17 | |
| 30*381*3.2(87°) | 2.7 | 19/16" x 15" x 1/8" (87°) | 5.95 | |
| 55*400*3.2 | 2.8 | 9/4" x 63/4" x 1/8" | 6.17 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
钩子板(间苯)常用于化工、电镀、污水处理等平台的边缘固定,与格栅、栏杆或型材连接,提供可靠的支撑与紧固。在需要高强度和耐腐蚀的场合,如海洋工程、石油平台,也能发挥其性能优势。具体适用性需根据实际工况评估,欢迎联系我们获取应用建议。
选型指导
选型时需确定钩子板的尺寸(A*B*T)、角度(如75°或斜边)以及安装方式,确保与现有结构匹配。间苯树脂赋予产品优于邻苯树脂的耐腐蚀性,适用于更苛刻的化学环境。如需详细规格与选型支持,请联系我们获取专业建议。
产品优势
采用间苯树脂,钩子板具有优异的耐腐蚀性和机械强度,重量轻、安装便捷,且绝缘无磁。玻璃纤维增强确保长期耐久性,适用于高负载和户外环境。我们可根据需求提供定制化解决方案,欢迎垂询。
询盘引导
欢迎联系我们获取详细规格、技术参数与报价。我们提供专业选型支持与定制服务,满足您的项目需求。请通过网站或邮箱联系,我们将尽快回复。

简体中文