Genius FRP  

   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Hollow board

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Hollow board

A1*T1*A2*T2*B*T3
A1*T1*A2*T2*B*T3

500*6*450*6*48.5*616.4

20" x 1/4" x 18" x 1/4" x 2" x 1/4"

36.2

500*6*450*6*48.5*918.5

20" x 1/4" x 18" x 1/4" x 2" x 3/8"

40.8

650*13*550*13*98.5*1252.5

51/2" x 1/2" x 173/8" x 1/2" x 4" x 1/2"

116

725*4.5*675*4.5*45*4.517.9

57/2" x 3/16" x 53/2" x 3/16" x 7/4" x 3/16"

39.5

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:    

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar  

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

空心板结构型材适用于对强度、跨度和耐腐蚀性有较高要求的工业平台、走道、护栏、支撑结构及设备框架等场合。其轻质高强的特性也常用于需要减轻自重或快速安装的改造项目。欢迎联系我们,根据您的具体工况推荐合适的规格。

选型指导

选型时请综合考虑荷载要求、跨度、使用环境(如腐蚀介质、温度)以及安装方式等因素。您可提供截面尺寸、长度及数量等信息,我们将协助您匹配适宜的型材规格。欢迎联系我们获取详细规格与报价。

产品优势

该空心板型材以玻璃纤维增强材料与树脂复合而成,具有轻质高强、耐腐蚀、绝缘及易加工等特点,能在多种苛刻环境下保持稳定性能。其结构设计兼顾承载效率与自重控制,便于运输和安装。欢迎联系我们了解更多材料特性与应用案例。

询盘引导

如需获取空心板结构型材的具体尺寸、重量、力学参数或定制方案,请直接联系我们。我们可根据您的项目需求提供选型建议与商务支持。欢迎联系我们获取详细规格与报价。

立即联系我们,我们将有专业人员为您服务。