结构型材-方管(间苯)
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Square tube | A*B*T1*T2 | A*B*T1*T2 | ||
| ST25A | 25*25*3.2*3.2 | 0.53 | 1" x 1" x 1/8" x 1/8" | 1.17 |
| ST25B | 25*25*6.4*6.4 | 0.9 | 1" x 1" x 1/4" x 1/4" | 1.98 |
| ST32A | 32*32*3.2*3.2 | 0.7 | 5/4" x 5/4" x 1/8" x 1/8" | 1.54 |
| ST32B | 32*32*6.4*6.4 | 1.24 | 5/4" x 5/4" x 1/4" x 1/4" | 2.73 |
| ST38A | 38*38*3.2*3.2 | 0.85 | 3/2" x 3/2" x 1/8" x 1/8" | 1.87 |
| ST38B | 38*38*5*5 | 1.25 | 3/2" x 3/2" x 3/16" x 3/16" | 2.76 |
| ST38C | 38*38*6.4*6.4 | 1.54 | 3/2" x 3/2" x 1/4" x 1/4" | 3.4 |
| ST44A | 44*44*3.2*3.2 | 1.01 | 7/4" x 7/4" x 1/8" x 1/8"
| 2.23 |
| ST44B | 44*44*6.4*6.4 | 1.83 | 7/4" x 7/4" x 1/4" x 1/4"
| 4.03 |
| ST50A | 50*50*3.2*3.2 | 1.14 | 2" x 2" x 1/8" x 1/8" | 2.51 |
| ST50B | 50*50*3.5*3.5 | 1.24 | 2" x 2" x 1/8" x 1/8" | 2.73 |
| ST50C | 50*50*4*4 | 1.42 | 2" x 2" x 3/16" x 3/16"
| 3.13 |
| ST50D | 50*50*5*5 | 1.74 | 2" x 2" x 3/16" x 3/16" | 3.84 |
| ST50E | 50*50*6.4*6.4 | 2.12 | 2" x 2" x 1/4" x 1/4" | 4.67 |
| ST54A | 54*54*3.2*3.2 | 1.24 | 9/4" x 9/4" x 1/8" x 1/8" | 2.73 |
| ST54B | 54*54*4.8*4.8 | 1.78 | 9/4" x 9/4" x 3/16" x 3/16" | 3.92 |
| ST60A | 60*60*5*5 | 2.1 | 19/8" x 19/8" x 3/16" x 3/16"
| 4.63 |
| ST64A | 64*64*3.2*3.2 | 1.48 | 5/2" x 5/2" x 1/8" x 1/8" | 3.26 |
| ST64B | 64*64*4.4*4.4 | 1.97 | 5/2" x 5/2" x 3/16" x 3/16"
| 4.34 |
| ST64C | 64*64*6.4*6.4 | 2.8 | 5/2" x 5/2" x 1/4" x 1/4"
| 6.17 |
| ST76A | 76*76*3.2*3.2 | 1.77 | 3" x 3" x 1/8" x 1/8"
| 3.9 |
| ST76B | 76*76*5*5 | 2.7 | 3" x 3" x 3/16" x 3/16" | 5.95 |
| ST76C | 76*76*6.4*6.4 | 3.39 | 3" x 3" x 1/4" x 1/4" | 7.47 |
| ST76D | 76*76*9.5*9.5 | 4.89 | 3" x 3" x 3/8" x 3/8" | 10.8 |
| ST89A | 89*89*6.4*6.4 | 3.95 | 7/2" x 7/2" x 1/4" x 1/4" | 8.71 |
| ST101A | 101*101*3.2*3.2 | 2.38 | 4" x 4" x 1/8" x 1/8"
| 5.25 |
| ST101B | 101*101*5*5 | 3.61 | 4" x 4" x 3/16" x 3/16"
| 7.96 |
| ST101C | 101*101*6.4*6.4 | 4.61 | 4" x 4" x 1/4" x 1/4" | 10.2 |
| ST152A | 152*152*6.4*6.4 | 7.1 | 6" x 6" x 1/4" x 1/4" | 15.7 |
| ST152B | 152*152*9.5*9.5 | 10.4 | 6" x 6" x 3/8" x 3/8" | 22.9 |
| ST152C | 152*152*12.7*12.7 | 13.5 | 6" x 6" x 1/2" x 1/2" | 29.8 |
| STR25 | 25*25*3.175*3.175 | 0.7 | 1" x 1" x 1/8" x 1/8" | 1.54 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
间苯型方管适用于对耐腐蚀性有一定要求的承重与结构场合,如平台支撑、护栏骨架、格栅承重梁及化工、水处理等行业的框架构件。其玻璃纤维增强结构适合大跨度、高强度需求,欢迎联系我们说明具体工况以获取适配建议。
选型指导
选型时需综合考虑受力形式、跨度、支撑间距及使用环境,先确定方管的边长与壁厚,再确认树脂体系是否匹配现场介质条件。表中间苯型方管提供多种规格,如需更详细的力学参数与截面选用建议,欢迎联系我们。
产品优势
该结构型材以玻璃纤维为增强材料、树脂为基体,经拉挤工艺成型,具有较好的物理性能与耐腐蚀性,适用于高强度、大跨度结构。间苯树脂体系在耐腐蚀与结构承载之间提供平衡,具体性能表现可结合使用环境向我方咨询。
询盘引导
如需获取间苯型方管的详细规格表、材质说明及价格信息,欢迎联系我们,我们将根据您的项目需求提供对应资料与报价。请告知所需尺寸、数量及使用环境,以便我们更快响应。