FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Riglet radian | Width*Thickness | Width*Thickness | ||
| FS50A | 50*3.2 | 0.29 | 2" x 1/8" | 0.64 |
| FS60A | 60*3.2 | 0.36 | 19/8" x 1/8" | 0.79 |
| FS70 | 70*4 | 0.54 | 19" x 3/16" | 1.19 |
| FS90A | 90*3.2 | 0.54 | 7/2" x 1/8" | 1.19 |
| FS100 | 100*3.2 | 0.6 | 4" x 1/8" | 1.32 |
| FS120 | 120*3 | 0.7 | 19/4" x 1/8" | 1.54 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
弧度平条(间苯树脂型)常用于需要弧面贴合与结构补强的部位,如罐体环向加强、管道支撑、弧形走道边框、护栏与平台收边等。间苯树脂体系使其在耐腐蚀与耐候要求较高的工况中更受青睐,适合化工、水处理、海洋及一般工业环境使用。具体适用工况可结合介质与荷载条件与我们确认。
选型指导
选型时建议先确认弧形半径与贴合面曲率,再根据跨度与承载要求确定宽度与厚度,最后结合安装方式(螺栓固定、粘接或与格栅/型材拼接)核对孔位与连接件。表中主推规格为常规参考,若现有规格与您的弧度或载荷不匹配,可联系我们按图按样定制。欢迎联系我们获取详细规格与报价。
产品优势
玻璃纤维增强与间苯树脂结合,赋予型材轻质高强、耐腐蚀、绝缘无磁、易切割安装等特性,适合替代部分金属型材以减轻自重并降低维护频率。拉挤成型工艺保证截面尺寸稳定、纤维连续分布,弧形结构在承载时受力更均匀。热膨胀系数与电绝缘性能等具体数据可索取资料确认。
询盘引导
如需确认弧度平条的规格、树脂体系或配套连接方案,请提供使用环境、弧形半径、长度与数量等信息,我们将协助匹配合适型号。价格、最小起订量与交期等商业条款欢迎联系我们获取详细规格与报价,样品与技术支持可一并沟通。