Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Round tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Round tube

D*T
D*T
RT2525*3.20.44

1" x 1/8"

0.97
RT26A26*30.42

1" x 1/8"

0.93
RT26B26*4.80.63

1" x 3/16"

1.39
RT32A32*3.20.55

5/4" x 1/8"

1.21
RT32B32*50.81

5/4" x 3/16"

1.79
RT32C32*60.96

5/4" x 1/4"

2.12
RT38A38*3.20.65

3/2" x 1/8"

1.43
RT38B38*40.81

3/2" x 3/16"

1.79
RT38C38*51

3/2" x 3/16"

2.2
RT38D38*6.41.18

3/2" x 1/4"

2.6
RT4141*4.50.98

13/8" x 3/16"

2.16
RT42A42*3.20.7

13/8" x 1/8"

1.54
RT42B42*51.11

13/8" x 3/16"

2.45
RT42C42*6.41.45

13/8" x 1/4"

3.2
RT4848*6.41.58

15/8" x 1/4"

3.48
RT50A50*3.20.84

2" x 1/8"

1.85
RT50B50*41.1

2" x 3/16"

2.43
RT50C50*51.34

2" x 3/16"

2.95
RT50D50*6.41.67

2" x 1/4"

3.68
RT50E50*3.50.96

2" x 1/8"

2.12
RT50.8A50.8*6.41.7

2" x 1/4"

3.75
RT50.8B50.8*3.20.86

2" x 1/8"

1.9
RT64A64*3.51.26

5/2" x 1/8"

2.78
RT64B64*6.42.38

5/2" x 1/4"

5.25
RT7575*4.21.8

3" x 3/16"

3.97
RT7676*6.42.64

3" x 1/4"

5.82
RT89A89*3.21.54

7/2" x 1/8"

3.4
RT89B89*52.51

7/2" x 3/16"

5.35
RT89C89*6.43.13

7/2" x 1/4"

6.9
RT9999*52.81

4" x 3/16"

6.19
RT101101*6.43.62

4" x 1/4"

7.98
RT114A114*3.22.12

9/2" x 1/8"

4.67
RT114B114*53.25

9/2" x 3/16"

7.17
RT114C114*6.44.11

9/2" x 1/4"

9.06
RT114D114*9.55.93

9/2" x 3/8"

13.07
RT150A150*3.22.81

6" x 1/8"

6.19
RT150B150*54.35

6" x 3/16"

9.59
RT150C150*6.45.5

6" x 1/4"

12.1
RT150D150*9.58

6" x 3/8"

17.6

Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

乙烯基圆管适用于对耐腐蚀与强度要求较高的场合,例如化工与污水处理平台的护栏、支撑杆,海洋与沿海工程的框架、爬梯,以及电力、轨道交通等领域的绝缘结构件。

在大跨度或轻量化要求明显的场景中,圆管可作为主受力杆件或桁架腹杆使用,便于与其他拉挤型材(如方管、角材、板材)组合设计。

选型指导

选型时请先确认使用环境的介质种类与浓度、工作温度、紫外暴露条件,以及结构所需的载荷形式(拉、压、弯)与连接方式,再据此选择合适的管径、壁厚和树脂体系。

不同直径与壁厚对应不同的截面惯性矩和承载能力,建议结合设计图纸或跨度要求确定规格;如需按工况推荐截面,欢迎联系我们提供参数并由技术团队协助选型。

产品优势

乙烯基树脂体系通常具有较好的耐腐蚀性和耐温表现,配合玻璃纤维增强后,圆管具备轻质高强、绝缘不导磁、免维护等复合材料典型优势。

拉挤工艺使纤维沿轴向连续分布,制品尺寸稳定、表面平整,便于切割、钻孔和现场安装,适合替代部分易锈蚀的金属管件。

询盘引导

如需了解具体规格、树脂类型、颜色、长度及包装方式,或希望获取样品与批量供货方案,欢迎联系我们。请提供使用环境、所需管径与壁厚的预期范围、数量及交货地,我们将安排技术对接与报价。

定制截面、特殊树脂体系及配套连接件均可沟通,详细规格与商务条款请以正式询盘回复为准。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数