Structural Profiles - Plum Tube (Vinyl Ester)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Plum tube | D1*D2*T | D1*D2*T | ||
CT32A | 19*32*6.4 | 1.11 |
3/4" x 5/4" x 1/4" | 2.45 |
CT34A | 19*34*7.5 | 1.3 | 3/4" x 5/4" x 5/16" | 2.87 |
CT32B | 25*32*3.5 | 0.66 | 1" x 5/4" x 1/8" | 1.46 |
CT42 | 29*42*6.4 | 1.35 | 9/8" x 13/8" x 1/4" | 2.98 |
CT45A | 28*45*8.5 | 1.86 | 9/8" x 7/4" x 5/16" | 4.1 |
CT45B | 32*45*6.4 | 1.1 | 5/4" x 7/4" x 1/4" | 2.43 |
CT51 | 51*36*7 | 1.75 | 2" x 3/2" x 1/4" | 3.86 |
CT90B | 71*90*9.5 | 5.7 | 11/4" x 7/2" x 3/8" | 12.6 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Quatrefoil tube (vinyl ester) is commonly used for structural supports, handrails, platform frames, and in chemical, marine, and other environments requiring corrosion resistance and strength. Its multi-lobed shape facilitates combination with other profiles, making it suitable for space-restricted or lightweight applications. For specific applications, please consult our technical team for selection based on your operating conditions.
Selection Guidance
When selecting, the cross-sectional dimensions and wall thickness of the tube should be determined based on load, span, corrosive environment, and installation method. Quatrefoil tube provides multi-directional load-bearing characteristics, making it suitable for combined stresses. Please contact us with your detailed operating conditions, and we will assist you in choosing the appropriate specifications.
Product Advantages
Fiberglass reinforced composite (FRP) quatrefoil tube is lightweight, high-strength, corrosion-resistant, insulating, and non-magnetic, and easy to process and install. The vinyl ester resin matrix further enhances chemical corrosion resistance, making it suitable for harsh environments. Compared with metal, it offers long service life and low maintenance cost.
Inquiry Guidance
For specific dimensions, weight, price, delivery time, and other information about quatrefoil tube, please contact us. We can provide customized solutions and professional advice according to your needs.
简体中文