结构型材-梅花管 (乙烯基)

结构型材-梅花管 (乙烯基)

价格面议

发起询价


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Plum tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Plum tube

D1*D2*T


D1*D2*T


CT32A

19*32*6.4

1.11

3/4" x 5/4" x 1/4"

2.45

CT34A

19*34*7.5

1.3

3/4" x 5/4" x 5/16"

2.87

CT32B

25*32*3.5

0.66

1" x 5/4" x 1/8"

1.46

CT42

29*42*6.4

1.35

9/8" x 13/8" x 1/4"

2.98

CT45A

28*45*8.5

1.86

9/8" x 7/4" x 5/16"

4.1

CT45B

32*45*6.4

1.1

5/4" x 7/4" x 1/4"

2.43

CT51

51*36*7

1.75

2" x 3/2" x 1/4"

3.86

CT90B

71*90*9.5

5.7

11/4" x 7/2" x 3/8"

12.6

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Quatrefoil tube (vinyl ester) is commonly used for structural supports, handrails, platform frames, and in chemical, marine, and other environments requiring corrosion resistance and strength. Its multi-lobed shape facilitates combination with other profiles, making it suitable for space-restricted or lightweight applications. For specific applications, please consult our technical team for selection based on your operating conditions.

Selection Guidance

When selecting, the cross-sectional dimensions and wall thickness of the tube should be determined based on load, span, corrosive environment, and installation method. Quatrefoil tube provides multi-directional load-bearing characteristics, making it suitable for combined stresses. Please contact us with your detailed operating conditions, and we will assist you in choosing the appropriate specifications.

Product Advantages

Fiberglass reinforced composite (FRP) quatrefoil tube is lightweight, high-strength, corrosion-resistant, insulating, and non-magnetic, and easy to process and install. The vinyl ester resin matrix further enhances chemical corrosion resistance, making it suitable for harsh environments. Compared with metal, it offers long service life and low maintenance cost.

Inquiry Guidance

For specific dimensions, weight, price, delivery time, and other information about quatrefoil tube, please contact us. We can provide customized solutions and professional advice according to your needs.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送