Structural Profiles - H-Beam (Orthophthalic Resin)

Structural Profiles - H-Beam (Orthophthalic Resin)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

H beam

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

H beam

A*B*T1*T2


A*B*T1*T2


HB76

76*76*6.4*6.4

2.67

3" x 3" x 1/4" x 1/4"

5.73

HB102A

102*102*6.4*6.4

3.59

4" x 4" x 1/4" x 1/4"

7.91

HB102B

102*102*8*8

4.5

4" x 4" x 5/16" x 5/16"

9.92

HB152A

152*152*6.4*6.4

5.43

6" x 6" x 1/4" x 1/4"

11.97

HB152B

152*152*9.5*9.5

8.1

6" x 6" x 3/8" x 3/8"

17.86

HB203A

203*203*9.5*9.5

10.8

8" x 8" x 3/8" x 3/8"

23.81

HB203B

203*203*12.7*12.7

14.4

8" x 8" x 1/2" x 1/2"

31.66

HB203C

203*203*6.4*6.4

7.5

8" x 8" x 1/4" x 1/4"

16.53

HB254A

254*254*9.5*9.5

13.6

10" x 10" x 3/8" x 3/8"

29.98

HB254B

254*254*12.7*12.7

18

10" x 10" x 1/2" x 1/2"

39.77

HB305

305*305*12.7*12.7

21.5

12" x 12" x 1/2" x 1/2"

47.4

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar 

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

FRP H-beams, being lightweight, high-strength and corrosion-resistant, are commonly used for structural support in corrosive environments such as chemical, marine and wastewater treatment applications, as well as for platform, walkway and frame systems requiring large spans and high strength. Please contact us for more specific application cases and suitable solutions.

Selection Guide

During selection, factors such as load requirements, span, service environment and connection method need to be considered comprehensively. H-beams with different section sizes and wall thicknesses are suitable for different load-bearing requirements. We recommend providing specific operating parameters, and our technical team will assist you in choosing the most suitable specification.

Product Advantages

This product is made of orthophthalic unsaturated polyester resin and glass fiber reinforcement, formed through the pultrusion process. It offers excellent physical properties, chemical corrosion resistance and electrical insulation, and is lightweight and easy to install, making it suitable for high-strength, large-span structural applications.

Inquiry Guide

For detailed specifications, technical parameters or customized solutions, please contact us. We can provide professional selection advice and quotations according to your project requirements, and we look forward to working with you.

Operating Environment

  • Pultruded FRP H-beams (HB76, HB102A, HB102B) are built on an orthophthalic resin matrix with glass fiber reinforcement, making them suited to humid, wet and chemically aggressive surroundings rather than dry indoor interiors alone.
  • Typical service locations are outdoor and semi-sheltered works where condensation, rain and airborne moisture are present, including chemical plant structures, water treatment areas, cooling tower frames and coastal or marine installations.
  • The glass fiber cloth package layer and resin-rich surfaces resist corrosion from acids, alkalis and salts in process areas and wash-down zones, so the beams can replace steel members where rust is a maintenance issue.
  • Because the profiles are non-conductive and non-magnetic, they also suit indoor electrical, instrumentation and electrolytic environments; for temperature limits, sustained loads or specific chemical media, contact Greenlogy TEC for the full parameter list.