FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
H beam | A*B*T1*T2 | A*B*T1*T2 | ||
HB76 | 76*76*6.4*6.4 | 2.67 | 3" x 3" x 1/4" x 1/4" | 5.73 |
HB102A | 102*102*6.4*6.4 | 3.59 | 4" x 4" x 1/4" x 1/4" | 7.91 |
HB102B | 102*102*8*8 | 4.5 |
4" x 4" x 5/16" x 5/16" | 9.92 |
HB152A | 152*152*6.4*6.4 | 5.43 |
6" x 6" x 1/4" x 1/4" | 11.97 |
HB152B | 152*152*9.5*9.5 | 8.1 |
6" x 6" x 3/8" x 3/8" | 17.86 |
HB203A | 203*203*9.5*9.5 | 10.8 |
8" x 8" x 3/8" x 3/8" | 23.81 |
HB203B | 203*203*12.7*12.7 | 14.4 |
8" x 8" x 1/2" x 1/2" | 31.66 |
HB203C | 203*203*6.4*6.4 | 7.5 |
8" x 8" x 1/4" x 1/4" | 16.53 |
HB254A | 254*254*9.5*9.5 | 13.6 |
10" x 10" x 3/8" x 3/8" | 29.98 |
HB254B | 254*254*12.7*12.7 | 18 |
10" x 10" x 1/2" x 1/2" | 39.77 |
HB305 | 305*305*12.7*12.7 | 21.5 |
12" x 12" x 1/2" x 1/2" | 47.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
FRP H-beams, being lightweight, high-strength and corrosion-resistant, are commonly used for structural support in corrosive environments such as chemical, marine and wastewater treatment applications, as well as for platform, walkway and frame systems requiring large spans and high strength. Please contact us for more specific application cases and suitable solutions.
Selection Guide
During selection, factors such as load requirements, span, service environment and connection method need to be considered comprehensively. H-beams with different section sizes and wall thicknesses are suitable for different load-bearing requirements. We recommend providing specific operating parameters, and our technical team will assist you in choosing the most suitable specification.
Product Advantages
This product is made of orthophthalic unsaturated polyester resin and glass fiber reinforcement, formed through the pultrusion process. It offers excellent physical properties, chemical corrosion resistance and electrical insulation, and is lightweight and easy to install, making it suitable for high-strength, large-span structural applications.
Inquiry Guide
For detailed specifications, technical parameters or customized solutions, please contact us. We can provide professional selection advice and quotations according to your project requirements, and we look forward to working with you.
Operating Environment
- Pultruded FRP H-beams (HB76, HB102A, HB102B) are built on an orthophthalic resin matrix with glass fiber reinforcement, making them suited to humid, wet and chemically aggressive surroundings rather than dry indoor interiors alone.
- Typical service locations are outdoor and semi-sheltered works where condensation, rain and airborne moisture are present, including chemical plant structures, water treatment areas, cooling tower frames and coastal or marine installations.
- The glass fiber cloth package layer and resin-rich surfaces resist corrosion from acids, alkalis and salts in process areas and wash-down zones, so the beams can replace steel members where rust is a maintenance issue.
- Because the profiles are non-conductive and non-magnetic, they also suit indoor electrical, instrumentation and electrolytic environments; for temperature limits, sustained loads or specific chemical media, contact Greenlogy TEC for the full parameter list.