LM (Coating) Sealed Comp. Wire Rope GB6X19 (9/9/1) FC
Please feel freely to contact with us for new price .
Product Details
6X19 (coating) sealed comp. wire rope (often referred to as 6X25) is available with both FC (fibre core) and IWRC (independent wire rope core). 6X19 (coating) sealed comp. wire rope can work from 1 tonne load up to 5 tonnes. It is used in the North Sea Oil industry .
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Drilling ropes
Elevator ropes
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Ground cables
Oil well / Oil field
Excavator rope / Scraper rope
Fishing rope
Drag ropes
Breaking Loads
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads | |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.36 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.43 | 70.7 | 7208 | 78.3 | 7982 |
| 12 | 0.52 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.61 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.7 | 114 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67556 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请根据实际应用场景的载荷要求、使用环境(如腐蚀性、温度)和安装方式来确定钢丝绳的直径、结构和表面处理(光面或镀锌)。建议参考国家标准GB/T 20118-2006,并欢迎联系我们获取详细规格与选型支持。
产品优势
本产品采用6X19压实填料结构,具有较高的破断拉力和抗疲劳性能,纤维芯(FC)提供良好的柔韧性。表面镀锌处理可增强耐腐蚀性,适用于多种工业场合。
询盘引导
如需获取详细技术参数、价格及交货期等信息,欢迎随时联系我们。请提供所需直径、长度、表面处理等具体要求,我们将为您提供专业报价和解决方案。