玻璃钢模塑格栅38*152H38 T型
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*152*38(mm)
Panel size available:
1220*3660 Length stress
Bearing bar thickness (Top/Bottom):15.0/8.0
Bearing bar center:38
Open Aera:62%
Approx Weight:18.6kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅38×152H38 T型广泛应用于化工、石油、电力、污水处理、海洋工程等领域的平台、走道、地沟盖板及楼梯踏步。其耐腐蚀、防滑、轻质高强的特性使其在潮湿、酸碱等恶劣环境中表现优异。如需针对您的具体工况推荐合适方案,欢迎联系我们获取详细规格与报价。
选型指导
选型时请综合考虑承载要求、跨距、腐蚀环境及安全等级。T型格栅具有更高的承载能力和防滑性能,适用于重载或对安全性要求较高的场合。您可提供具体使用条件,我们将协助您选择最合适的树脂类型和格栅规格。
产品优势
本产品采用不饱和聚酯树脂与无碱玻璃纤维模压成型,具有优异的耐腐蚀性、轻质高强、防滑绝缘、易于安装和维护等特点。相比传统金属格栅,其使用寿命更长,且无需频繁防腐处理,综合成本更低。
询盘引导
欢迎联系我们获取详细规格、技术参数及报价。我们可根据您的需求提供定制化解决方案,并为您提供专业的技术支持。
简体中文