玻璃钢模塑格栅25*25H50

玻璃钢模塑格栅25*25H50

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

Software - Sample 2 for three columns

Polished type

Software - Sample 3 for three columns

Shop sand type

25 25 H50

25*25*50(mm)

Panel size available:

1524*4000 Bidirectional force.

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:25

Open Aera:55%

Approx Weight:28.5kgs/m²

25 25 H50

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.

Software - Sample 1 for three columns


Software - Sample 2 for three columns


Software - Sample 3 for three columns



应用场景

玻璃钢模塑格栅25*25H50具有耐腐蚀、轻质高强、防滑等特性,适用于化工、电镀、水处理、海洋工程等行业的操作平台、走道、楼梯踏板及地沟盖板。其25mm网格与50mm厚度在承重与透水性之间取得平衡,适合中等荷载的工业环境。具体场景选型欢迎联系我们获取详细建议。

选型指导

选型时需确认树脂类型(如邻苯、间苯、乙烯基酯或双酚A型)以匹配耐腐蚀要求,并根据荷载、跨距选择格栅厚度与网格尺寸(本产品为25*25H50)。同时可考虑表面防滑处理(如加砂)及颜色定制。如需技术选型支持,欢迎联系我们获取详细规格与报价。

产品优势

本产品采用不饱和聚酯树脂与无碱玻璃纤维模压成型,具有优异的耐腐蚀性、抗老化性和电绝缘性,且重量轻、安装便捷、维护成本低。其结构设计兼顾承载与排水,适用于多种工业环境。欢迎联系我们获取详细规格与报价。