结构型材-工字梁

结构型材-工字梁

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation. 

I beam

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

I-beam

A*B*T1*T2


A*B*T1*T2


IB3215*32*6.4*40.510.59*1.26*0.25*0.161.12
IB38A30*38*3*30.531.18*1.5*0.12*0.121.17
IB45A45*9*180*125.41.77*0.35*7.09*0.4711.9
IB50A50*102*6.4*6.42.41.97*4.02*0.25*0.255.29
IB50B50*102*8*831.97*4.02*0.31*0.316.61
IB76A76*152*6.4*6.43.592.99*5.98*0.25*0.257.91
IB76B76*152*9.5*9.55.322.99*5.98*0.37*0.3711.73
IB102A102*203*9.5*9.57.24.02*7.99*0.37*0.3715.87
IB102B102*203*12.7*12.79.54.02*7.99*0.5*0.520.94
IB120120*240*12*1210.54.02*9.45*0.47*0.4723.15
IB127A127*254*9.5*9.595*10*0.37*0.3719.84
IB127B127*254*12.7*12.711.95*10*0.5*0.526.24
IB127C127*152*9.5*9.57.15*5.98*0.37*0.3715.65
IN127D127*152*12.7*12.79.25*5.98*0.5*0.520.28
IB152A152*305*9.5*9.510.75.98*12.01*0.37*0.3723.68
IB152B152*305*12.7*12.714.35.98*12.01*0.5*0.531.53

Markets  

Markets
  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Standard color

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Grass green,Yellow, Grey, Orange

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

Grass green,Yellow, Grey

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

Grass green,Yellow, Grey

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

结构型材-工字梁适用于对强度与跨距有要求的承重与支撑部位,例如平台走道、栈桥、设备支架、护栏骨架及腐蚀性环境中的结构框架。不同树脂体系与纤维铺层可适配多种工况,欢迎联系我们获取详细规格与报价。

选型指导

选型时需综合考虑载荷形式、跨距、支撑条件、使用环境及连接方式,据此确定截面尺寸与长度方向的要求。由于各工况差异较大,建议提供使用条件由我方协助确认合适型号,欢迎联系我们获取详细规格与报价。

产品优势

FRP工字梁以玻璃纤维增强材料与树脂复合而成,具有轻质高强、耐腐蚀、绝缘无磁、易于切割与现场加工等特点,便于在金属型材易锈蚀的场合替代使用。具体性能表现随配方与规格而变,欢迎联系我们获取详细规格与报价。

询盘引导

如需确认截面规格、长度、颜色、树脂类型或配套连接方案,请提供图纸或使用条件,我方将据此给出建议。欢迎联系我们获取详细规格与报价,也可就样品与批量供货事宜进一步沟通。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数