FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Flat tube | A*B*T1*T2 | A*B*T1*T2 | ||
| FT44 | 44*25*3.2*3.2 | 0.8 | 7/4" x 1" x 1/8" x 1/8" | 1.76 |
| FT50A | 51*25*3*3 | 0.79 | 2" x 1" x 1/8" x 1/8" | 1.74 |
| FT50B | 51*25*6.4*6.4 | 1.54 | 2" x 1" x 1/4" x 1/4" | 3.4 |
| FT76 | 76*35*3*6 | 1.55 | 3" x 11/8" x 1/8" x 1/4" | 3.42 |
| FT80 | 80*60*5*5 | 2.5 | 25/8" x 19/8" x 3/16" x 3/16" | 5.51 |
| FT91A | 91*38*4*4 | 1.78 | 7/2" x 3/2" x 3/16" x 3/16" | 3.92 |
| FT112A | 112*91*6.4*6.4 | 4.46 | 9/2" x 7/2" x 1/4" x 1/4" | 9.83 |
| FT120 | 120*45*3*3 | 2 | 19/4" x 7/4" x 1/8" x 1/8" | 4.41 |
| FT175 | 175*50*9*9 | 7 | 55/8" x 2" x 3/8" x 3/8" | 15.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-扁管(间苯)常用于对强度与耐腐蚀性有要求的承重与支撑结构,如平台骨架、护栏立柱、走道支撑及设备框架等。间苯树脂体系适用于潮湿、酸碱或户外暴露等环境,可在多种工况下替代部分金属型材。具体适用场景与安装方式欢迎联系我们沟通。
选型指导
选型时可结合受力方向、跨度、连接方式与环境介质,在扁管的截面尺寸、壁厚及树脂体系之间进行权衡。本页尺寸表列出各规格的截面与单位重量,可据此初步比对,但实际承载与挠度需按工程设计确认。如需针对具体项目的选型建议,欢迎联系我们获取详细规格与报价。
产品优势
拉挤成型工艺使玻璃纤维沿轴向连续排布,赋予扁管较高的轴向强度与刚度,同时具备FRP材料轻质、耐腐蚀、非磁性、绝缘及易加工等特性。间苯树脂体系进一步提升了对潮湿与化学环境的耐受能力,便于现场切割、钻孔与螺栓连接。具体性能表现欢迎垂询。
询盘引导
如您需要确定规格、数量、长度或其他定制要求,欢迎联系我们获取详细规格与报价。请提供使用环境、受力条件与所需截面尺寸,我们将据此提供选型建议与商务条款。