Pultruded Grating HL-5020

Pultruded Grating HL-5020

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

HL5020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 50%

Approx Weight (With three-core shoots): 52.24kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

(mm)

15030045075015003000450060007500
6000.040.080.10.180.370.711.081.421.79
7500.060.120.20.330.651.31.952.623.27
9000.10.220.330.551.12.193.274.375.47
12000.260.510.771.282.565.127.6810.212.8
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

(mm)

4509501450245048509800145001950024400
6000.040.080.140.220.450.891.341.792.21
7500.10.20.30.511.022.033.074.085.1
9000.20.410.611.022.054.16.148.1910.2
12000.651.281.933.216.412.8---------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating HL-5020 is suitable for industrial platforms, walkways, trench covers and equipment operating surfaces that require load-bearing capacity, corrosion resistance and slip resistance. Typical applications include chemical, water treatment, electroplating and marine engineering environments that are wet or corrosive, and it can also be used in structural parts requiring insulation or weight reduction. Please contact us to confirm suitability for your specific application.

Selection Guidance

When selecting, consider the load-bearing span, the corrosive media in the service environment, whether flame retardancy is required and the installation method, then match the appropriate resin type and grating thickness. Different resin systems offer different advantages in corrosion resistance and flame retardancy. Please contact us for detailed specifications and selection advice. We can recommend a suitable configuration based on your operating conditions.

Product Advantages

Pultruded grating is assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods. It features light weight, high strength, corrosion resistance and resistance to rusting. Compared with traditional metal grating, it is free from electrochemical corrosion, has lower maintenance costs, and is easy to cut and install on site. Its overall structure is stable and suitable for long-term exposure to harsh environments.

Inquiry Guide

For specific specifications, resin options and commercial terms of Pultruded Grating HL-5020, please contact us for detailed specifications and a quotation. Please provide your service environment, load-bearing requirements and dimensional needs, and we will match a suitable solution and reply as soon as possible.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send