FRP Molded Grating 25*100H25

FRP Molded Grating 25*100H25

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 100 H25

25*100*25(mm)

Panel size available:

1007*3007 Width stress     

Bearing bar thickness (Top/Bottom):7.0/5.5

Bearing bar center:25

Open Aera:67%

Approx Weight:13kgs/m²

Liner load

Liner load(units:mm)

Deflcvtion

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

Span( mm)

75150300450600750

Load

3000.330.480.740.991.271.529942
6000.861.733.455.186.918.644305
7501.402.725.117.169.5511.93589
9002.414.728.1812.416.520.63216
Uniform load

Uniform load(units:mm)

Deflcvtion

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span( mm)

2404809801450245036504880
3000.280.380.530.711.04---1.91
6000.911.853.685.549.22---18.5
9003.636.612.618.5---------
10508.0114.9---------------
25 100 H25

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP Molded Grating 25*100H25 is suitable for platforms, walkways, stair treads and trench covers in chemical, petroleum, power, marine engineering and other fields. Its corrosion resistance, slip resistance, light weight and high strength make it perform well in harsh environments such as humid and acid-alkali conditions.

Selection Guide

When selecting, consider load-bearing requirements, span, corrosive environment and safety level. 25*100H25 indicates a grating thickness of 25 mm and a mesh size of 100 mm. Different resin types (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.) can be selected according to specific needs to meet corrosion resistance or flame retardant requirements.

Product Advantages

FRP molded grating features light weight, high strength, corrosion resistance, slip resistance, insulation and maintenance-free performance, with a long service life and easy installation, effectively reducing long-term costs.

Inquiry Guide

For more detailed specifications or technical parameters of FRP Molded Grating 25*100H25, or to obtain a quotation, please contact us. We will provide you with professional technical support and customized services.

Operating Environment

  • This FRP molded grating is built on unsaturated polyester resin, which supports use in both indoor and outdoor installations where moisture and humid air are present.
  • The phenolic resin option (MP-5) provides low toxicity and high flame retardant properties, making it suitable for fire-sensitive environments.
  • With its fiberglass reinforcement and resin matrix, the grating is appropriate for areas exposed to corrosive media, as the material resists chemical attack.
  • Typical applications include walkways and platforms where the grating must withstand foot traffic and environmental exposure without losing structural integrity.