拉挤格栅 T-1810
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 18%
Approx Weight (With three-core shoots): 13.8kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
(mm) | 300 | 500 | 800 | 1500 | 2000 | 2500 | Load |
| 400 | 0.4 | 0.67 | 1.07 | 2 | 2.67 | 3.34 | 5900 |
| 600 | 1.24 | 2.06 | 3.3 | 8.25 | --- | --- | 2300 |
| 800 | 2.76 | 4.59 | 7.35 | 13.8 | --- | --- | 2300 |
| 1000 | 5.16 | 8.6 | 13.8 | --- | --- | --- | 2200 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
(mm) | 300 | 500 | 800 | 1500 | 2000 | 2500 | Load |
| 400 | 0.1 | 0.17 | 0.27 | 0.5 | 0.67 | 0.83 | 29600 |
| 600 | 0.46 | 0.77 | 1.24 | 2.32 | 3.1 | 3.87 | 12700 |
| 800 | 1.38 | 2.3 | 3.67 | 6.89 | 9.18 | 11.5 | 7300 |
| 1000 | 3.22 | 5.37 | 8.6 | --- | --- | --- | 4600 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 T-1810 适用于对承载和耐腐蚀有要求的工业平台、走道、楼梯踏板、沟盖板及污水处理、化工、海洋工程等场合。其结构由拉挤“I”型或“T”型承重条与实心管或棒作为连接杆组装而成,具有轻质高强、耐腐蚀、防滑等特点。具体适用环境请结合工况咨询我们。
选型指导
选型时需考虑树脂类型(如邻苯型、间苯型、乙烯基型、酚醛型等)以满足不同的耐腐蚀和阻燃要求,同时确定格栅的厚度、网格尺寸、承载等级和表面防滑处理。不同树脂体系对应不同的耐化学性和阻燃性能,例如酚醛型具有低毒高阻燃特性。欢迎联系我们获取详细规格与选型建议。
产品优势
拉挤格栅 T-1810 采用拉挤工艺成型,纤维含量高,具有优异的单向强度和高刚度。相较于模塑格栅,拉挤格栅在承载方向上的强度更高,适合长跨距应用。产品耐腐蚀、免维护、绝缘无磁,且安装便捷。具体性能参数请咨询我们。
询盘引导
如需了解拉挤格栅 T-1810 的详细规格、技术参数、价格及交货期,欢迎联系我们。请提供您的具体应用需求,我们将为您提供专业的技术支持和报价。
简体中文
English