拉挤格栅 I-4015
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 38mm
Open Area: 40%
Approx Weight (With three-core shoots): 22kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.12 | 0.25 | 0.51 | 0.76 | 1.52 | 2.79 | 26215 |
| 600 | 0.29 | 0.51 | 1.02 | 1.78 | 3.05 | 5.84 | 19661 |
| 900 | 1.02 | 1.27 | 2.29 | 5.32 | 9.38 | 17.8 | 12705 |
| 1200 | 2.95 | 3.59 | 5.57 | 9.4 | 19.1 | 38.9 | 9086 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.25 | 0.45 | 0.76 | 1.67 | 2.42 | 4.83 | 114645 |
| 600 | 0.61 | 1.18 | 2.32 | 4.59 | 5.96 | 9.62 | 64506 |
| 900 | 1.92 | 3.79 | 6.33 | 11.2 | 15.5 | --- | 27757 |
| 1200 | 4.96 | 9.64 | --- | --- | --- | --- | 14905 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 I-4015 采用拉挤“I”型承载条与实心管或棒作为连接杆装配而成,适用于对承载与耐腐蚀有要求的平台、走道、地沟盖板及各类工业操作面。在化工、水处理、电镀、海洋及一般腐蚀性介质环境中,可按具体工况选用不同树脂体系。欢迎联系我们说明使用环境,以便确认适配方案。
选型指导
选型时建议先明确介质种类与浓度、环境温度、载荷形式及安装支撑跨度,再据此选择树脂类型(如酚醛型、乙烯基型等)与格栅厚度、承载条间距。不同树脂在阻燃与耐腐蚀性能上各有侧重,具体规格与承载数据请与我们联系获取。
产品优势
拉挤格栅以连续拉挤型材为承载单元,具有轻质高强、耐腐蚀、不导电、免维护等特点,便于切割与现场安装,可减少后期维护成本。其表面可做成防滑形式,提升行走安全性。有关具体性能表现,欢迎联系我们获取详细资料。
询盘引导
如需了解拉挤格栅 I-4015 的详细规格、树脂选项、承载能力与报价,欢迎联系我们,提供使用工况与尺寸需求,我们将为您推荐合适方案并给出报价。
简体中文