LM Wire Rope GB1x19
Please feel freely to contact with us for new price .
产品详情
1x19 wire rope is one of the most common wire rope structures. 1x19 has excellent fracture strength , tensile properties and beautiful appearance. It has been widely used in the whole shipbuilding industry, mining industry, construction industry and other fields.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Railing
Fixed rigging
Mast brace
Guard rail
Structural member
Supporting Rope
Marine Engineering
Sewage treatment
Breaking Loads
Diameter
| Weight
|
Min Breaking Loads(1570 Mpa)
|
Min Breaking Loads(1570 Mpa)
|
mm | kg/m | KN |
Kg |
| 2 | 0.02 | 3.14 | 320 |
| 2.5 | 0.03 | 4.9 | 499 |
| 3 | 0.04 | 7.06 | 719 |
| 4 | 0.08 | 12.6 | 1284 |
| 5 | 0.12 | 19.6 | 1998 |
| 6 | 0.18 | 28.2 | 2875 |
| 7 | 0.24 | 34.8 | 3548 |
| 8 | 0.31 | 45.5 | 4639 |
| 9 | 0.4 | 57.6 | 5873 |
| 10 | 0.49 | 71.1 | 7250 |
| 11 | 0.59 | 86 | 8769 |
| 12 | 0.7 | 102 | 10401 |
| 14 | 0.96 | 139 | 14174 |
| 16 | 1.25 | 182 | 18558 |
| 19 | 1.76 | 212 | 21617 |
| 22 | 2.36 | 285 | 29061 |
| 26 | 3.3 | 398 | 40584 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.

简体中文