LM Compacted Non-rotating Wire Rope GB19X7 (6/1)
Please feel freely to contact with us for new price .
产品详情
19x7 is available in both galvanised and ungalvanised finish,including 17x7,18x7.For further flexibility and other performance characteristics we also supply 32X7, 35X7 and 37X7.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Offshore crane rope
Deck crane rope
Pillar crane rope
Whip hoist rope
Main hoist rope
Main hoist rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.63 | 91.7 | 9349 | 102 | 10388 |
| 13 | 0.74 | 108 | 10972 | 120 | 12191 |
| 14 | 0.86 | 125 | 12725 | 139 | 14139 |
| 15 | 0.99 | 143 | 14608 | 159 | 16231 |
| 16 | 1.13 | 163 | 16621 | 181 | 18467 |
| 18 | 1.43 | 206 | 21035 | 229 | 23373 |
| 20 | 1.76 | 255 | 25970 | 283 | 28855 |
| 22 | 2.13 | 308 | 31423 | 342 | 34915 |
| 24 | 2.53 | 367 | 37396 | 407 | 41551 |
| 26 | 2.97 | 430 | 43889 | 478 | 48765 |
| 28 | 3.45 | 499 | 50901 | 554 | 56556 |
| 30 | 3.96 | 573 | 58432 | 637 | 64924 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请先明确起重设备的额定载荷、滑轮与卷筒直径、使用环境(如海上、潮湿或腐蚀工况)及所需安全系数,再结合直径与最小断裂荷载对照表确定合适规格。不同表面处理(光面或镀锌)与结构(如17x7、18x7、32x7等)适用场景不同,建议将具体工况告知我们,由技术人员协助匹配。
产品优势
该19x7压实型不旋转钢丝绳采用压实工艺,结构紧密,在起升与吊装过程中具有较好的抗旋转性能,有助于减少负载摆动。产品可按需提供光面或镀锌表面处理,并符合GB/T 20118-2006标准,适用于海上起重机、甲板起重、立柱吊车及主提升等场景。
询盘引导
如需了解不同直径、表面处理及1770MPa或1960MPa强度等级的具体规格与报价,欢迎联系我们获取详细技术资料与商务方案。我们可根据您的工况推荐合适结构,并确认供货与交付安排。