拉挤格栅 I-4010

拉挤格栅 I-4010

价格面议

发起询价


欢迎询价。

Genius FRP  

Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface

Software - Sample 2 for three columns

Smooth surface

Software - Sample 3 for three columns

Antiskid groove surface

I 4010
Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 50%
Approx Weight (With three-core shoots): 17.8kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.380.581.022.034.067.6216593
6000.951.562.544.578.8917.512959
9003.094.647.7315.530.9---8639
12005.848.8914.729.559.2---6420
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

4500.851.763.225.637.2512.172325
6001.913.717.5612.916.5---42515
9006.5712.823.3---------18863
120014.5---------------10507

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories

I 4010

Application Scenarios

Pultruded grating I-4010 is suitable for platforms, walkways, trench covers and stair treads that require both load-bearing capacity and corrosion resistance, and is commonly used in chemical, water treatment, power and marine engineering environments. Different resin systems correspond to different media and temperature conditions; please contact us to confirm the specific applicability based on your operating conditions.

Selection Guide

When selecting, first clarify the load-bearing requirements, span, corrosive media and flame retardant requirements, and then choose the resin type as well as the grating thickness and mesh size accordingly. In the table, systems such as OFR, IFR, VEFR and phenolic each have their own emphasis in flame retardancy and corrosion resistance. Please contact us for detailed specifications and selection advice.

Product Advantages

Pultruded grating is assembled with pultruded I-shaped and T-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, so it has strong longitudinal load-bearing capacity and high stiffness, and is lightweight, corrosion-resistant and easy to cut and install. Its surface is anti-slip and requires low maintenance, making it suitable as a replacement for metal grating.