Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25%
| OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65%
| E |
Filler |
8% | ATH,PR |
Others | 2%
| --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 50%
Approx Weight (With three-core shoots): 17.8kg/m²

Liner load(units:mm)
Spacing |
kg/m |
kg/m |
kg/m |
kg/m |
kg/m |
kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.38 | 0.58 | 1.02 | 2.03 | 4.06 | 7.62 | 16593 |
| 600 | 0.95 | 1.56 | 2.54 | 4.57 | 8.89 | 17.5 | 12959 |
| 900 | 3.09 | 4.64 | 7.73 | 15.5 | 30.9 | --- | 8639 |
| 1200 | 5.84 | 8.89 | 14.7 | 29.5 | 59.2 | --- | 6420 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.85 | 1.76 | 3.22 | 5.63 | 7.25 | 12.1 | 72325 |
| 600 | 1.91 | 3.71 | 7.56 | 12.9 | 16.5 | --- | 42515 |
| 900 | 6.57 | 12.8 | 23.3 | --- | --- | --- | 18863 |
| 1200 | 14.5 | --- | --- | --- | --- | --- | 10507 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded grating I-4010 is suitable for platforms, walkways, trench covers and stair treads that require both load-bearing capacity and corrosion resistance, and is commonly used in chemical, water treatment, power and marine engineering environments. Different resin systems correspond to different media and temperature conditions; please contact us to confirm the specific applicability based on your operating conditions.
Selection Guide
When selecting, first clarify the load-bearing requirements, span, corrosive media and flame retardant requirements, and then choose the resin type as well as the grating thickness and mesh size accordingly. In the table, systems such as OFR, IFR, VEFR and phenolic each have their own emphasis in flame retardancy and corrosion resistance. Please contact us for detailed specifications and selection advice.
Product Advantages
Pultruded grating is assembled with pultruded I-shaped and T-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, so it has strong longitudinal load-bearing capacity and high stiffness, and is lightweight, corrosion-resistant and easy to cut and install. Its surface is anti-slip and requires low maintenance, making it suitable as a replacement for metal grating.