Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




50*50*50(mm)
Panel size available:
1800*4000,1524*4000,1220*3660,
1220*2440,915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:50
Open Aera:78%
Approx Weight:20.8kgs/m²

Liner load(units:mm)
Span in (mm) | Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 5.7 | 30 | 11.8 |
| 600 | 15.1 | 21 | 14.9 |

Uniform load(units:mm)
Span in (mm) | Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 1.4 | 154 | 11.8 |
| 600 | 5.7 | 73 | 14.9 |
| 800 | 1.6 | 35 | 16.5 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



Application Scenarios
The FRP molded grating 50×50 H50 light duty type is suitable for walkways, operating platforms, trench covers, stair treads and light-load supporting applications in various corrosive environments. Its mesh structure and light-duty design facilitate cutting and installation, and it can be flexibly adjusted to on-site dimensions. Please contact us to confirm the specific operating conditions.
Selection Guidance
When selecting, please take into account load requirements, span, the corrosiveness and flame retardant requirements of the service environment, and the installation method. This product is a 50×50 mm mesh, 50 mm thick light-duty specification. If you need different load ratings, resin systems or colors, please contact us for detailed specifications and selection advice.
Product Advantages
Molded from unsaturated polyester resin and fiberglass, it features corrosion resistance, light weight and high strength, slip resistance and insulation, and maintenance-free operation. It is also water-permeable, light-transmitting and easy to process on site. Different resin systems vary in their emphasis on flame retardancy and chemical resistance, and can be selected as needed. For more performance details, please contact us.
Inquiry Guidance
For detailed specifications, resin options, color customization, packaging and delivery arrangements of this product, please contact us for a detailed quotation and technical support. Please provide your application scenario and quantity requirements, and we will recommend a suitable solution for you.
简体中文
English