Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




50*50*50(mm)
Panel size available:
1800*4000,1524*4000,1220*3660,
1220*2440,915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):8.0/6.0
Bearing bar center:50
Open Aera:78%
Approx Weight:23.7kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
Span( mm) | 150 | 300 | 450 | 600 | 750 | 1500 | Load |
| 300 | 0.31 | 0.41 | 0.48 | 0.64 | 1.04 | 1.45 | 21727 |
| 600 | 0.51 | 0.81 | 1.23 | 1.75 | 3.33 | 4.27 | 11713 |
| 900 | 1.12 | 2.24 | 3.2 | 5.16 | 6.58 | 13.5 | 7780 |
| 1200 | 1.33 | 2.61 | 5.98 | 9.95 | 11.9 | --- | 5834 |

Uniform load(units:mm)
Deflcvtion |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
Span( mm) | 240 | 480 | 980 | 1450 | 2450 | 3650 | 4880 |
| 300 | 0.25 | 0.28 | 0.33 | 0.38 | 0.48 | 0.74 | --- |
| 600 | 0.38 | 0.58 | 0.97 | 1.37 | 2.13 | 4.12 | --- |
| 900 | 1.19 | 2.11 | 3.94 | 5.77 | 9.45 | 18.6 | --- |
| 1200 | 2.41 | 4.93 | 9.96 | 15 | 16.8 | 21.6 | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
玻璃钢模塑格栅广泛应用于化工、石油、电力、污水处理、海洋工程等领域的操作平台、走道、楼梯踏板及地沟盖板。其耐腐蚀、防滑、轻质高强的特性使其在潮湿、酸碱等恶劣环境中表现优异。
选型指导
选型时需综合考虑承载要求、跨距、腐蚀环境及防火等级。不同树脂类型(如邻苯、间苯、乙烯基、酚醛)适用于不同腐蚀介质和温度条件。欢迎联系我们获取详细规格与选型建议,我们将根据您的工况提供合适方案。
产品优势
玻璃钢模塑格栅具有优异的耐腐蚀性、轻质高强、防滑、绝缘及免维护等特点,使用寿命长,安装简便。与传统金属格栅相比,可显著降低维护成本,尤其适用于高腐蚀环境。
询盘引导
如需了解更多产品信息、技术参数或获取报价,欢迎联系我们。请提供具体应用场景、尺寸要求及数量,我们将尽快为您提供专业支持。
简体中文
English