玻璃钢模塑格栅40*40H25
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




40*40*25(mm)
Panel size available:
1247*4047,1007*4047,1007*3007
Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:40
Open Aera:67%
Approx Weight:12.3kgs/m²

Liner load(units:mm)
Span in (mm) | Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 4.7 | 19 | 7.14 |
| 600 | 13.2 | 13 | 8.55 |

Uniform load(units:mm)
Span in (mm) | Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 1.2 | 100 | 7.14 |
| 600 | 4.9 | 45 | 8.55 |
| 800 | 14.8 | 26 | 9.02 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
玻璃钢模塑格栅40*40H25广泛应用于化工、石油、电力、污水处理等行业的操作平台、楼梯踏板、地沟盖板及围栏。其耐腐蚀特性使其适用于潮湿、酸碱等腐蚀性环境。欢迎联系我们了解更详细的应用案例。
选型指导
选型时需综合考虑承载要求、跨距、腐蚀环境及防火等级。不同树脂类型(如邻苯、间苯、乙烯基、酚醛)适用于不同工况,例如酚醛型具有优异阻燃性能。如需专业选型建议,请联系我们的技术团队获取详细规格与报价。
产品优势
玻璃钢模塑格栅具有轻质高强、耐腐蚀、防滑、绝缘及免维护等优点。其网格结构设计便于安装和切割,且使用寿命长,可降低长期维护成本。欢迎联系我们获取更多产品优势信息。
询盘引导
如需获取玻璃钢模塑格栅40*40H25的详细规格、技术参数或报价,请通过网站联系我们。我们可根据您的需求提供定制化解决方案,并竭诚为您服务。
简体中文