玻璃钢模塑格栅38*100H50仿拉挤
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*100*50(mm)
Panel size available:
1220*3660 Length stress
Bearing bar thickness (Top/Bottom):8.0/5.0
Bearing bar center:38
Open Aera:62%
Approx Weight:15.3kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅38*100H50仿拉挤适用于对防滑、耐腐蚀和承载有要求的平台、走道、地沟盖板及设备操作面,常见于化工、水处理、电力与一般工业环境。其38×100mm网格与50mm厚度带来仿拉挤外观的平整表面,便于在潮湿、易积液或需频繁冲洗的场合使用。若您有具体工况,欢迎联系我们确认适配方案。
选型指导
选型时建议先明确树脂体系(如邻苯、间苯、乙烯基或双酚A型)与阻燃要求,再结合承载跨度、支撑方式及安装固定形式确定格栅厚度与网格规格。38×100H50仿拉挤在承载与开孔率之间取得平衡,适合需要仿拉挤表面效果又希望保持模塑格栅整体性的项目。欢迎联系我们获取详细规格与选型建议。
产品优势
该格栅以不饱和聚酯树脂为基体、玻璃纤维为增强材料,具备轻质高强、耐腐蚀、防滑及绝缘等特点,且表面仿拉挤处理使外观更接近拉挤型材。模塑成型的一体化结构减少了拼接与维护需求,适用于长期暴露于腐蚀性介质或户外环境的场合。具体性能表现可结合您的使用条件进一步评估。
询盘引导
如需了解玻璃钢模塑格栅38*100H50仿拉挤的详细规格、树脂选型、颜色及包装运输等信息,欢迎联系我们获取详细规格与报价。请提供使用环境、承载要求与数量,我们将协助您匹配适合的产品方案。
简体中文