玻璃钢模塑格栅26*26H38
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




26*26*38(mm)
Panel size available:
1150*4011 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.0/5.0
Bearing bar center:25
Open Aera:60%
Approx Weight:19.5kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅26*26H38适用于对防滑、耐腐蚀与承载有要求的平台、走道、地沟盖板、楼梯踏步及设备操作面等场合,常见于化工、水处理、电力、海洋工程与一般工业车间。具体工况的适配性可结合介质、载荷与安装方式与我们沟通确认。
选型指导
选型时建议先明确使用环境的腐蚀介质与阻燃要求,再确认承载需求与支撑跨距,以便在邻苯型、间苯型、乙烯基酯型或双酚A型等树脂体系及不同网格、厚度规格间做出匹配。欢迎联系我们提供工况条件,我们将协助推荐合适的格栅型号与结构方案。
产品优势
模塑成型工艺使格栅整体一次成型,纤维与树脂分布均匀,兼具轻质高强、耐腐蚀、防滑绝缘与便于切割安装等特点,日常维护成本较低。相较于传统金属格栅,其在潮湿、酸碱等环境下更不易锈蚀,使用寿命更长。
询盘引导
如需了解玻璃钢模塑格栅26*26H38的详细规格、树脂体系选项、颜色与表面处理方式,欢迎联系我们获取详细规格与报价。请提供使用环境、承载要求与所需数量等信息,我们将尽快为您提供针对性的选型建议与商务方案。