玻璃钢模塑格栅25*100H30
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*30(mm)
Panel size available:
1007*3007 Width stress
Bearing bar thickness (Top/Bottom):7.0/5.5
Bearing bar center:25
Open Aera:67%
Approx Weight:15.6kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅具有优异的耐腐蚀性、轻质高强和防滑性能,广泛应用于化工、石油、电力、海洋工程等领域的操作平台、走道、地沟盖板及楼梯踏板等。其开放式网格结构便于液体和气体通过,减少积水和风阻,适用于对安全性和耐久性要求较高的工业环境。如需了解具体应用案例,欢迎联系我们。
选型指导
选型时需考虑使用环境的腐蚀性、承载要求、防火等级及颜色等因素。例如,在强腐蚀环境中建议选用间苯或乙烯基酯树脂;在防火要求高的场合可选用酚醛树脂(如MP-5)。不同网格尺寸和厚度影响承载能力,请根据实际需求咨询我们的技术团队获取专业建议。
产品优势
玻璃钢模塑格栅采用高强度玻璃纤维与树脂整体模塑成型,具有轻质高强、耐腐蚀、防滑、绝缘、无磁性、易安装等特点,使用寿命长,维护成本低。其独特的网格设计可有效排水、防积尘,并可根据客户需求定制颜色和尺寸,满足多样化工业需求。
询盘引导
如需获取详细规格、技术参数、样品或报价,欢迎随时联系我们。我们的专业团队将根据您的具体需求提供定制化解决方案,确保为您提供最合适的产品与服务。