玻璃钢模塑格栅 19*19H38
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




19*19*38(mm)
Panel size available:
1524*4000,1220*3660,1220*2440,
915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.5/5.0
Bearing bar center:19
Open Aera:40%
Approx Weight:23.5kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
Span( mm) | 150 | 300 | 450 | 600 | 750 | 1500 | Load |
| 300 | 0.36 | 0.48 | 0.61 | 0.76 | 0.89 | 1.06 | 17116 |
| 600 | 0.66 | 1.25 | 1.85 | 2.46 | 3.07 | 8.48 | 8718 |
| 900 | 1.8 | 3.68 | 5.56 | 7.42 | 9.3 | 13.8 | 5817 |
| 1200 | 4.75 | 9.68 | 14.6 | 19.6 | 21.2 | --- | 3755 |

Uniform load(units:mm)
| Deflcvtion | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² |
| Span(mm) | 240 | 480 | 980 | 1450 | 2450 | 3650 | 4880 |
| 300 | 0.09 | 0.19 | 0.38 | 0.49 | 0.78 | 1.05 | --- |
| 600 | 0.43 | 0.81 | 1.55 | 2.31 | 3.84 | 5.74 | --- |
| 900 | 1.70 | 3.45 | 6.96 | 10.5 | 17.5 | 23.3 | --- |
| 1200 | 5.97 | 12.2 | 24.5 | 32.6 | 38.7 | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
玻璃钢模塑格栅19*19H38适用于对防滑、耐腐蚀和承载有要求的通行平台、走道、地沟盖板及设备操作面,常见于化工、水处理、电镀、海洋工程等潮湿或腐蚀性环境。不同树脂体系可针对具体介质与工况选择,欢迎联系我们说明使用环境以获取匹配建议。
选型指导
选型时可从树脂类型、格栅厚度、网格尺寸与承载需求四个维度综合考虑:腐蚀性介质决定树脂体系,跨度与荷载决定厚度与支撑方式。由于涉及具体工况参数,欢迎联系我们提供使用条件,由技术人员协助确认合适规格。
产品优势
模塑格栅采用树脂与玻璃纤维一体成型,具有轻质高强、耐腐蚀、防滑及绝缘等特点,且便于切割安装与后期维护。相比传统金属格栅,其在潮湿和腐蚀环境中更不易锈蚀,有助于降低长期维护成本。
询盘引导
如需了解19*19H38模塑格栅的详细规格、树脂选项、包装方式及交货安排,欢迎联系我们获取详细规格与报价。请提供使用环境、所需尺寸与数量,我们将据此给出针对性方案。