Structural Profiles - Square Tube (Vinyl Ester)

Structural Profiles - Square Tube (Vinyl Ester)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Square tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Square tube

A*B*T1*T2


A*B*T1*T2


ST25A25*25*3.2*3.20.53

1" x 1" x 1/8" x 1/8"

1.17
ST25B25*25*6.4*6.40.9

1" x 1" x 1/4" x 1/4"

1.98
ST32A32*32*3.2*3.20.7

5/4" x 5/4" x 1/8" x 1/8"

1.54
ST32B32*32*6.4*6.41.24

5/4" x 5/4" x 1/4" x 1/4"

2.73
ST38A38*38*3.2*3.20.85

3/2" x 3/2" x 1/8" x 1/8"

1.87
ST38B38*38*5*51.25

3/2" x 3/2" x 3/16" x 3/16"

2.76
ST38C38*38*6.4*6.41.54

3/2" x 3/2" x 1/4" x 1/4"

3.4
ST44A44*44*3.2*3.21.01

7/4" x 7/4" x 1/8" x 1/8"

2.23
ST44B44*44*6.4*6.41.83

7/4" x 7/4" x 1/4" x 1/4"

4.03
ST50A50*50*3.2*3.21.14

2" x 2" x 1/8" x 1/8"

2.51
ST50B50*50*3.5*3.51.24

2" x 2" x 1/8" x 1/8"

2.73
ST50C50*50*4*41.42

2" x 2" x 3/16" x 3/16"

3.13
ST50D50*50*5*51.74

2" x 2" x 3/16" x 3/16"

3.84
ST50E50*50*6.4*6.42.12

2" x 2" x 1/4" x 1/4"

4.67
ST54A54*54*3.2*3.21.24

9/4" x 9/4" x 1/8" x 1/8"

2.73
ST54B54*54*4.8*4.81.78

9/4" x 9/4" x 3/16" x 3/16"

3.92
ST60A60*60*5*52.1

19/8" x 19/8" x 3/16" x 3/16"

4.63
ST64A64*64*3.2*3.21.48

5/2" x 5/2" x 1/8" x 1/8"

3.26
ST64B64*64*4.4*4.41.97

5/2" x 5/2" x 3/16" x 3/16"

4.34
ST64C64*64*6.4*6.42.8

5/2" x 5/2" x 1/4" x 1/4"

6.17
ST76A76*76*3.2*3.21.77

3" x 3" x 1/8" x 1/8"

3.9
ST76B76*76*5*52.7

3" x 3" x 3/16" x 3/16"

5.95
ST76C76*76*6.4*6.43.39

3" x 3" x 1/4" x 1/4"

7.47
ST76D76*76*9.5*9.54.89

3" x 3" x 3/8" x 3/8"

10.8
ST89A89*89*6.4*6.43.95

7/2" x 7/2" x 1/4" x 1/4"

8.71
ST101A101*101*3.2*3.22.38

4" x 4" x 1/8" x 1/8"

5.25
ST101B101*101*5*53.61

4" x 4" x 3/16" x 3/16"

7.96
ST101C101*101*6.4*6.44.61

4" x 4" x 1/4" x 1/4"

10.2
ST152A152*152*6.4*6.47.1

6" x 6" x 1/4" x 1/4"

15.7
ST152B152*152*9.5*9.510.4

6" x 6" x 3/8" x 3/8"

22.9
ST152C152*152*12.7*12.713.5

6" x 6" x 1/2" x 1/2"

29.8
STR2525*25*3.175*3.1750.7

1" x 1" x 1/8" x 1/8"

1.54

 Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Vinylester square tubes are suitable for platforms, handrails and support structures in chemical, papermaking, electroplating and other environments with acid and alkali corrosion, and are also commonly used where electromagnetic insulation and lightweight high strength are required. For corrosion resistance performance under specific environments, please contact us to confirm based on the medium and working conditions.

Selection Guide

During selection, the side length and wall thickness of the square tube can be determined according to load, span and connection method, and general-purpose and vinylester types can be distinguished to meet different corrosion resistance requirements. If you provide the working conditions and load conditions, we can assist in recommending suitable specifications. Welcome to contact us for detailed specifications and quotations.

Product Advantages

This square tube uses glass fiber as reinforcement and resin as binder, and is formed by pultrusion. It features lightweight high strength, corrosion resistance and insulation, making it suitable for replacing some metal profiles. The surface can be treated in different ways as needed; please communicate with us for specific available options.

Inquiry Guide

If you need information such as the size range, weight, color and packaging of the square tube, welcome to contact us for detailed specifications and quotations. Please provide the required specifications, quantity and usage environment, and we will reply as soon as possible.

Operating Environment

  • Vinyl resin square tube from this FRP structural shapes line is built for outdoor and indoor industrial settings where moisture, salt spray or chemical splash would corrode steel — the pultruded glass fiber reinforcement carries the load while the vinyl resin matrix shields it.
  • Typical placement is on walkways, platforms, handrail frames and support structures in plants, water treatment areas and coastal installations, where the square tube stays dimensionally stable instead of rusting or swelling.
  • Because the pultruded profile is molded through heat-curing and traction, it resists UV exposure and repeated wet-dry cycling better than untreated metal, making it suitable for open-air spans that see sun, rain and washdown.
  • For highly concentrated acids or elevated temperatures, contact us with your service conditions so the appropriate vinyl resin formulation and wall thickness can be confirmed against your project.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send