Structural Profiles - Plum Tube (Isophthalic)

Structural Profiles - Plum Tube (Isophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Plum tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Plum tube

D1*D2*T


D1*D2*T


CT32A

19*32*6.4

1.11

3/4" x 5/4" x 1/4"

2.45

CT34A

19*34*7.5

1.3

3/4" x 5/4" x 5/16"

2.87

CT32B

25*32*3.5

0.66

1" x 5/4" x 1/8"

1.46

CT42

29*42*6.4

1.35

9/8" x 13/8" x 1/4"

2.98

CT45A

28*45*8.5

1.86

9/8" x 7/4" x 5/16"

4.1

CT45B

32*45*6.4

1.1

5/4" x 7/4" x 1/4"

2.43

CT51

51*36*7

1.75

2" x 3/2" x 1/4"

3.86

CT90B

71*90*9.5

5.7

11/4" x 7/2" x 3/8"

12.6

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

With its corrosion resistance, high strength and lightweight properties, the isophthalic cloverleaf tube is widely used in structural support and frame systems in chemical, marine, wastewater treatment and other fields. Its unique cloverleaf cross-section design reduces weight while maintaining load-bearing capacity, making it suitable for applications with demanding span and corrosion resistance requirements.

Selection Guide

Selection should take into account load conditions, span, service environment and installation method. Cloverleaf tubes in different specifications have different cross-sectional dimensions and weights, meeting diverse structural needs. Contact us for detailed specifications and selection advice; our technical team will provide professional support based on your specific working conditions.

Product Advantages

The isophthalic resin system gives the product excellent corrosion resistance and weather resistance, extending service life. Formed by the pultrusion process, it has a high fiber content and outstanding longitudinal strength while remaining lightweight for easy transport and installation. In addition, FRP material is insulating and non-magnetic, making it suitable for applications with electromagnetic interference requirements.

Inquiry Guide

For detailed product parameters, prices and supply information, please contact us at any time. Please provide specific specifications, quantity and service environment, and we will provide a professional quotation and technical support as soon as possible.

Operating Environment

  • This structural plum tube, pultruded from glass fiber reinforced material with resin as the adhesive, is intended for service in industrial settings where high strength over large spans is required. Its pultruded FRP construction allows it to be considered for both indoor and outdoor installations, depending on the surrounding conditions.
  • The isophthalic resin matrix (as indicated by "间苯" in the product name) is typically chosen for environments where moderate chemical exposure or moisture may be present. It is suitable for use in areas where conventional steel profiles would require additional protection against corrosion.
  • As with all FRP structural shapes, the operating temperature and humidity range of the plum tube depends on the specific resin formulation and application. For detailed recommendations on temperature limits, chemical resistance or UV exposure, please contact us with your project conditions.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send